[0016] A production method of home textile pearl cotton, which uses polyester / regenerated cellulose "∞ conjoined spiral crimped" superfine fiber, low melting point hot-melt fiber and kapok fiber to process and produce home textile pearl cotton;
[0017] The specific operation steps are as follows:
[0018] (1) Weigh 1kg of polyester / regenerated cellulose "∞ conjoined spiral crimp" superfine fiber and 200g of low-melting point hot-melt fiber, put them into a cylindrical barrel, and mix them by hand with a fork; you can also use a machine to mix them. Cotton, mix the two fibers evenly;
[0019] (2) Feed the mixed fiber after mixing into the pearl cotton ball machine, rub it, sprinkle 100g kapok evenly in the kneading process, rub it for 5 minutes, insert the kapok fiber into the gap therein, and form a support;
[0020] (3) Under the condition of 150°C, bake for 5s; after baking, the low-melting-point hot-melt fiber melts, and several connection points are formed between the ka...
specific Embodiment 2
[0026] A production method of home textile pearl cotton, which uses polyester / regenerated cellulose "∞ conjoined spiral crimped" superfine fiber, low melting point hot-melt fiber and kapok fiber to process and produce home textile pearl cotton;
[0027] The specific operation steps are as follows:
[0028] (1) Weigh 1kg of polyester / regenerated cellulose "∞ conjoined spiral crimped" superfine fiber and 250g of low-melting point hot-melt fiber, put them into a cylindrical barrel, and mix them by hand with a fork; you can also use a machine to mix them. Cotton, mix the two fibers evenly;
[0029] (2) Feed the mixed fiber after mixing into the pearl cotton ball machine, rub it, sprinkle 200g kapok evenly in the kneading process, knead it for 10 minutes, insert the kapok fiber into the gap therein, and form a support;
[0030] (3) Bake at 180°C for 10s; after baking, the low-melting-point hot-melt fiber melts, and several connection points are formed between the kapok and the sup...
specific Embodiment 3
[0036] A production method of home textile pearl cotton, which uses polyester / regenerated cellulose "∞ conjoined spiral crimped" superfine fiber, low melting point hot-melt fiber and kapok fiber to process and produce home textile pearl cotton;
[0037] The specific operation steps are as follows:
[0038] (1) Weigh 1kg of polyester / regenerated cellulose "∞ conjoined spiral crimped" superfine fiber and 220g of low-melting point hot-melt fiber, put them into a cylindrical barrel, and mix them by hand with a fork; you can also use a machine to mix them. Cotton, mix the two fibers evenly;
[0039] (2) Feed the mixed fiber after mixing into the pearl cotton ball machine, rub it, sprinkle 150g kapok evenly in the kneading process, knead it for 8 minutes, insert the kapok fiber into the gap therein, and form a support;
[0040] (3) Baking for 8s at 170°C; after baking, the low-melting-point hot-melt fiber melts, and several connection points are formed between the kapok and the sup...