Embodiment 1
[0015] Embodiment 1: A kind of PVC profile that is used for wear-resistant indoor floor, wherein the ratio of parts by weight of each component is: K65 type vinyl chloride resin powder 77 parts by weight, metal soap stabilizer 2.75 parts by weight, wherein stearic acid 1.375 parts by weight of calcium, 0.6875 parts by weight of zinc stearate, 0.6875 parts by weight of barium stearate, 2 parts by weight of pentaerythritol, 0.25 parts by weight of microcrystalline paraffin, 10 parts by weight of impact modifier ABS terpolymer, ethylene-propylene rubber 2 parts by weight, 6 parts by weight of kaolin.
[0016] Put the raw materials into the mixer and mix them. The mixing temperature of the mixer is 100°C. Add the cooled mixed raw materials into the extruder for extrusion and extrusion molding. The outlet temperature of the extruder is 120°C.
Embodiment 2
[0017] Embodiment 2: A kind of PVC profile that is used for wear-resistant indoor floor, wherein the ratio of parts by weight of each component is: 84 parts by weight of K65 type vinyl chloride resin powder, 1.85 parts by weight of metal soap stabilizer, wherein stearic acid 0.925 parts by weight of calcium, 0.4625 parts by weight of zinc stearate, 0.4625 parts by weight of barium stearate, 0.5 parts by weight of xylitol, 0.5 parts by weight of mannitol, 0.15 parts by weight of microcrystalline paraffin, impact modifier ABS terpolymer 8 parts by weight, 1 part by weight of ethylene propylene rubber, and 4 parts by weight of kaolin.
[0018] Put the raw materials into the mixer and mix them. The mixing temperature of the mixer is 105°C. Add the cooled mixed raw materials into the extruder for extrusion and extrusion molding. The outlet temperature of the extruder is 125°C.
Embodiment 3
[0019] Embodiment 3: A kind of PVC profile that is used for wear-resisting indoor floor, wherein the ratio of parts by weight of each component is: 80 parts by weight of K65 type vinyl chloride resin powder, 2.4 parts by weight of metal soap stabilizer, wherein stearic acid 1.2 parts by weight of calcium, 0.6 parts by weight of zinc stearate, 0.6 parts by weight of barium stearate, 0.8 parts by weight of pentaerythritol, 0.8 parts by weight of xylitol, 0.2 parts by weight of microcrystalline paraffin, impact modifier ABS terpolymer 9 Parts by weight, 1.8 parts by weight of ethylene propylene rubber, and 5 parts by weight of kaolin.
[0020] Put the raw materials into the mixer and mix them. The mixing temperature of the mixer is 102°C. Add the cooled mixed raw materials into the extruder for extrusion and extrusion molding. The outlet temperature of the extruder is 123°C.