Delay composition with long-term healing per second and production method of delay composition
A production method and technology of delayed medicine, applied in the direction of explosives, etc., can solve the problems of complex production process and poor precision, and achieve the effect of simple production process, less waste water and easy operation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0033] The following components were weighed according to mass ratio: 35% molybdenum powder; 51.95% barium chromate; 8% potassium perchlorate; 5% calcium fluoride; 0.05% binder. The binder adopts polyvinyl alcohol aqueous solution with a mass concentration of 2.5%.
Embodiment 2
[0035] The following components were weighed according to mass ratio: molybdenum powder 36%; barium chromate 52.6%; potassium perchlorate 5%; calcium fluoride 6%; binder 0.4%. The binder is an aqueous solution of polyvinyl alcohol with a mass concentration of 1.0%.
Embodiment 3
[0037] The following components were weighed according to mass ratio: molybdenum powder 35%; barium chromate 54%; potassium perchlorate 5%; calcium fluoride 5.9%; binder 0.1%. The binder is an aqueous solution of polyvinyl alcohol with a mass concentration of 2%.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com