Inorganic coating preventing incrustation from being generated and method used for preventing incrustation from being generated on surface of heating element
A technology of inorganic coating and scaling, applied in the direction of coating, etc., can solve the problems of low thermal conductivity, poor non-stickiness, low hardness, etc., and achieve the effect of low sintering temperature
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0050] Embodiment 1: including 10% inorganic resin, 10% organic solvent, 20% alumina, 20% titanium dioxide, 5% whisker silicon, 5% kaolin and 30% film-forming accelerator. The inorganic resin, organic solvent, alumina, titanium dioxide, whisker silicon and kaolin are sequentially added to the grinder for grinding and mixing to form the first medicament. The grinder is 500 rpm, and the grinding time is 45 minutes; The agent is the second agent mixed with the first agent before construction.
[0051] A method for preventing scaling by using an inorganic coating on the surface of a heating element for preventing scaling, characterized in that it comprises the following steps:
[0052]S10: The raw materials with the following mass percentages: 10% inorganic resin, 10% organic solvent, 20% alumina, 20% titanium dioxide, 5% whisker silicon, 5% kaolin and 30% film-forming The accelerator is sent into the mixed rolling paint tank and mixed evenly, the rotating speed of the mixed roll...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com