A kind of production process of oil-proof forming paper
A production process and technology for forming paper, which is applied in the field of papermaking, and can solve problems such as difficult control of concentration, incomplete pulping degree of pulping, and inability of surface glue to play its respective functions, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] A production process of oil-proof formed paper, which comprises the following steps: wood pulp disintegration, beating, pulp blending, papermaking and other processes;
[0021] Wood pulp disintegration: Add Wuzhen brand bleached kraft softwood pulp and Bukuo brand bleached kraft hardwood pulp with a weight ratio of 80:20 to the hydropulper;
[0022] Beating: After being mixed and crushed by a hydraulic pulper, it is poured into the knocking tank, soaked for about two hours, and then double-disc milled for beating. Control at 4.5%; pulping is divided into two times, the half pulp is 50 ° SR, wet weight 8g, the finished pulp is 76 ° SR, wet weight 5.0g, and the beaten slurry is poured into the pulp tank;
[0023] Mixing pulp: Pour cassava cationic starch with a substitution degree of 0.033 and a boiled concentration of 5% into the pulp mixing tank together with the slurry in the pulping tank, and the dosage of cassava cationic starch is 10kg / ton of paper;
[0024] After ...
Embodiment 2
[0029] A production process of oil-proof formed paper, which comprises the following steps: wood pulp disintegration, beating, pulp blending, papermaking and other processes;
[0030] Wood pulp disintegration: Add Wuzhen brand bleached kraft softwood pulp and Bukuo brand bleached kraft hardwood pulp with a weight ratio of 90:10 to the hydropulper;
[0031] Beating: After being mixed and crushed by a hydraulic pulper, it is poured into the knocking tank, soaked for about two hours, and then double-disc milled for beating. It is controlled at 4.0%; pulping is divided into two times, the degree of beating of the half pulp is 53°SR, the wet weight is 6g, the degree of beating of the pulp is 74°SR, and the wet weight is 4.0g, and the beaten pulp is poured into the pulping tank;
[0032] Mixing pulp: Pour cassava cationic starch with a substitution degree of 0.033 and a boiling concentration of 5% into the pulp mixing tank together with the slurry in the pulping tank, and the dosage...
Embodiment 3
[0038] A production process of oil-proof formed paper, which comprises the following steps: wood pulp disintegration, beating, pulp blending, papermaking and other processes;
[0039] Wood pulp disintegration: Add Wuzhen brand bleached kraft softwood pulp and Bukuo brand bleached kraft hardwood pulp with a weight ratio of 85:15 to the hydropulper;
[0040] Beating: After being mixed and crushed by a hydraulic pulper, it is poured into the knocking tank, soaked for about two hours, and then double-disc milled for beating. It is controlled at 4.2%; pulping is divided into two times, the half pulp is 52°SR, wet weight 6g, the pulping degree is 75°SR, wet weight is 4.5g, and the beaten pulp is poured into the pulp tank;
[0041] Mixing pulp: Pour cassava cationic starch with a substitution degree of 0.033 and a boiled concentration of 5% into the pulp mixing tank together with the slurry in the pulping tank, and the dosage of cassava cationic starch is 12kg / ton of paper;
[0042]...