A method of fixing silk screen
A technology for fixing silk screen and silk screen printing, which is applied in the post-processing of printing, printing, printing devices, etc., which can solve the problem of silk screen falling off and achieve the effect that it is not easy to fall off
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0021] A method of fixing the silk screen of this embodiment, that is, the "reconstructed surface" silk screen method, comprises the following steps:
[0022] Step 1: Make a leak board, and a gap corresponding to the size and specification of the silk screen is opened on the leak board;
[0023] Step 2, add 0.06 wt % leather fixative to the primer used in tanning and stir;
[0024] Step 3, put the stencil close to the substrate so that the gap of the stencil is aligned with the printing position, use a brush corresponding to the size of the gap of the stencil or a sponge wrapping cloth to dip in the primer obtained in step 2 to smear on the printing position, and silk screen;
[0025] Step 4: Dry the substrate at the screen printing position at 55°C for 6 minutes.
Embodiment 2
[0027] A method of fixing the silk screen of this embodiment, that is, the "reconstructed surface" silk screen method, comprises the following steps:
[0028] Step 1: Make a leak board, and a gap corresponding to the size and specification of the silk screen is opened on the leak board;
[0029] Step 2, add 0.07 wt % leather fixative to the primer used in tanning and stir;
[0030] Step 3, put the stencil close to the substrate so that the gap of the stencil is aligned with the printing position, use a brush corresponding to the size of the gap of the stencil or a sponge wrapping cloth to dip in the primer obtained in step 2 to smear on the printing position, and silk screen;
[0031] Step 4: Dry the substrate at the screen printing position at 60°C for 7 minutes.
Embodiment 3
[0033] A method of fixing the silk screen of this embodiment, that is, the "reconstructed surface" silk screen method, comprises the following steps:
[0034] Step 1: Make a leak board, and a gap corresponding to the size and specification of the silk screen is opened on the leak board;
[0035] Step 2, add 0.08 wt % leather fixative to the primer used in tanning and stir evenly;
[0036] Step 3, put the stencil close to the substrate so that the gap of the stencil is aligned with the printing position, use a brush corresponding to the size of the gap of the stencil or a sponge wrapping cloth to dip in the primer obtained in step 2 to smear on the printing position, and silk screen;
[0037] Step 4: Dry the substrate at the screen printing position at 60°C for 8 minutes.