Embodiment 1
[0022] A kind of Sendon-4 nanoemulsion is prepared by the following method:
[0023] S1. Weigh: 1.1g ethyl acetate, 3.75g absolute ethanol, 6.25g Tween-80, 13.75ml Sendon-4 extract, 0.05g preservative (methylparaben), 0.05g ascorbic acid, 0.5g g azone
[0024] S2. Mix Tween-80 and ethyl acetate and stir evenly. After the water temperature is kept at 40-60 degrees, stop stirring, add anhydrous ethanol, continue stirring for 30 minutes, stop stirring, and add dropwise with a plastic tip dropper and heat it to 40 degrees in advance. -60 degrees of Sendeng-4 extract, after 3-8 hours of dropwise addition, keep it at 40-60 degrees for 1 hour, turn off the heating, reduce to room temperature, add other auxiliary materials, and stir evenly, that is, it is obtained.
Embodiment 2
[0026] A kind of Sendon-4 nanoemulsion is prepared by the following method:
[0027] S1. Weigh: 1.1g ethyl acetate, 3.75g absolute ethanol, 6.25g Tween-80, 2.1ml Sendon-4 extract, 3ml alcohol infusion, 8.65ml distilled water, 0.05g preservative (paraben methyl ester), 0.05g ascorbic acid, 0.5g azone.
[0028] S2. Mix Tween-80 and ethyl acetate and stir evenly. After the water temperature is kept at 40-60 degrees, stop stirring, add anhydrous ethanol, continue stirring for 30 minutes, stop stirring, and add dropwise with a plastic tip dropper and heat it to 40 degrees in advance. -60 degrees of Sendeng-4 extract, after 3-8 hours of dropwise addition, keep it at 40-60 degrees for 1 hour, turn off the heating, reduce to room temperature, add other auxiliary materials, and stir evenly, that is, it is obtained.
[0029] The nanoemulsion obtained in Example 1 and Example 2 was centrifuged at 12,000 r·min-1 for 20 min, and the nanoemulsion was still clear and uniform in appearance, ...