Embodiment 1
[0017] A diatomite decorative material for purifying air, the diatomite decorative material comprises the following components in parts by weight: 8 parts of diatomite, 5 parts of PE reinforcing agent, 15 parts of powder filler, redispersible glue 1 part of powder, 15 parts of gel material, 1 part of dispersion medium, 8 parts of silver ion agent, 2 parts of sericite powder, 2 parts of hydrophobic powder, 5 parts of nano titanium dioxide, 1 part of modifier, 3 parts of anti-crack cellulose , 15 parts of deionized water.
[0018] A preparation method of a diatomite decorative material for purifying air, comprising the following steps:
[0019] Step 1: Add nano-titanium dioxide into water at 30-50°C, and disperse until uniform by ultrasonic to obtain a nano-titanium dioxide solution;
[0020] Step 2: adding a modifying agent to the nano-titanium dioxide solution obtained in step 1, and stirring and dispersing to obtain a modified nano-titanium dioxide solution;
[0021] Step 3...
Embodiment 2
[0024] A diatomite decorative material for purifying air, the diatomite decorative material comprises the following components in parts by weight: 15 parts of diatomite, 6 parts of PE reinforcing agent, 25 parts of powder filler, redispersible glue 2 parts of powder, 20 parts of gel material, 1.3 parts of dispersion medium, 10 parts of silver ion agent, 4 parts of sericite powder, 3 parts of hydrophobic powder, 9 parts of nano titanium dioxide, 2 parts of modifier, 5 parts of anti-crack cellulose , 30 parts of deionized water.
[0025] A preparation method of a diatomite decorative material for purifying air, comprising the following steps:
[0026] Step 1: Add nano-titanium dioxide into water at 30-50°C, and disperse until uniform by ultrasonic to obtain a nano-titanium dioxide solution;
[0027] Step 2: adding a modifying agent to the nano-titanium dioxide solution obtained in step 1, and stirring and dispersing to obtain a modified nano-titanium dioxide solution;
[0028]...
Embodiment 3
[0031] A diatomite decorative material for purifying air, the diatomite decorative material comprises the following components in parts by weight: 20 parts of diatomite, 8 parts of PE reinforcing agent, 35 parts of powder filler, redispersible glue 3 parts of powder, 30 parts of gel material, 1.8 parts of dispersion medium, 12 parts of silver ion agent, 7 parts of sericite powder, 5 parts of hydrophobic powder, 12 parts of nano titanium dioxide, 2.5 parts of modifier, 7 parts of anti-crack cellulose , 40 parts of deionized water.
[0032] A preparation method of a diatomite decorative material for purifying air, comprising the following steps:
[0033] Step 1: Add nano-titanium dioxide into water at 30-50°C, and disperse until uniform by ultrasonic to obtain a nano-titanium dioxide solution;
[0034] Step 2: adding a modifying agent to the nano-titanium dioxide solution obtained in step 1, and stirring and dispersing to obtain a modified nano-titanium dioxide solution;