Silver cyanide drying method
A technology of silver cyanide and sodium cyanide, applied in drying, drying machine, drying solid materials and other directions, can solve the problems of low safety, large heat loss, and high toxicity, so as to improve drying efficiency and avoid Waste of heat energy, effect of ensuring safety
Patent Information
- Authority / Receiving Office
- CN · China
- Current Assignee / Owner
- Publication Date
- 2021-07-30
Abstract
Description
technical field
[0001] The invention relates to the technical field of silver cyanide drying, in particular to a silver cyanide drying method. Background technique
[0002] Silver cyanide is white or light gray powder, odorless, tasteless, and highly toxic. Inhalation of silver cyanide can cause cyanide poisoning, headache, fatigue, dyspnea, convulsions, coma, and even death. Inhalation of isoamyl nitrite Detoxification, this product is mainly used for medicine and silver plating. It should be stored in a cool and ventilated warehouse, away from fire and heat sources. The package should be sealed. It should be stored separately from oxidants, acids and food chemicals. Do not store them together. Suitable materials should be prepared to contain the leakage. Silver cyanide is usually used in medicine, silver plating, as a protective coating, autoclave lining, electrical contacts, and electroplating of aircraft engine bearings. Ether chlorine and alcohol are used to make steric...
Examples
Embodiment 1
[0023] The invention provides a technical solution:
[0024] A method for drying silver cyanide, comprising the following steps:
[0025] Step 1: take quantitative silver metal and nitric acid by weighing equipment, then weigh quantitative water and quantitative sodium cyanide, and then put them into respective storage containers;
[0026] Step 2: Put the weighed quantitative silver and nitric acid into the mixing container at the same time, dissolve the silver completely, then add the quantitative water weighed in step 1 to dilute, add the weighed quantitative sodium cyanide, close the shielding cover of the mixing vessel after completing the reaction;
[0027] Step 3: Separating and washing the precipitate obtained in step 2, and then putting the precipitate into a holding container;
[0028] Step 4: Put the sediment holding container washed in step 3 into the heating device for heating. When putting it into the holding container, put it on the top of the built-in vibratio...