Medicinal ointment containing zinc conjugated linoleate and sodium humate
A technology of conjugated linoleic acid and sodium humate, applied in medical preparations containing active ingredients, ointment delivery, antineoplastic drugs, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] First weigh the components according to the mass ratio: cis-9, trans-11-conjugated linoleic acid zinc salt: sodium brown humic acid and sodium black humic acid mixture: medical white oil: distilled water: Span: tert-butyl para Hydroquinone, the ratio of which is 30.15:31.6:28.14:10:0.1:0.01;
[0027] Heat 28.14 parts of medical white oil to 50°C, add 30.15 parts of cis-9, trans-11-conjugated linoleic acid zinc salt and 0.01 part of antioxidant tert-butylhydroquinone under stirring conditions to obtain liquid A;
[0028] Add 31.6 parts of the mixture of sodium brown humate and sodium black humate into 10 parts of distilled water, stir to dissolve, and heat to 70°C to obtain liquid B;
[0029] Then add liquid B and 0.1 part of surfactant Span to liquid A, emulsify with a powerful emulsifier for 0.5 hour, and cool to room temperature to obtain a medicinal ointment containing zinc conjugated linoleic acid and sodium humate .
Embodiment 2
[0031] First, each component is weighed according to the mass ratio: trans-9, cis-11-conjugated linoleic acid zinc salt and trans-10, a mixture of cis-12-conjugated linoleic acid zinc salt: sodium palmate: Medical white oil: distilled water: sucrose polyester: tert-butyl p-hydroxyanisole, the ratio is 30:40:24.77:5:0.2:0.03;
[0032] Heat 24.77 parts of medical white oil to 70°C, add trans-9, cis-11-conjugated linoleic acid zinc salt and trans-10, 15 parts of cis-12-conjugated linoleic acid zinc salt and Antioxidant tert-butyl p-hydroxyanisole 0.03 part obtains A liquid;
[0033] Add 40 parts of sodium brown humate to 5 parts of distilled water, stir to dissolve, and heat to 60°C to obtain liquid B;
[0034] Then add liquid B and 0.2 parts of surfactant sucrose polyester to liquid A, emulsify with a strong emulsifier for 3 hours, and cool to room temperature to obtain a drug containing zinc conjugated linoleic acid and sodium humate. Use ointment.
Embodiment 3
[0036] First weigh each component according to the mass ratio: trans-10, cis-12-conjugated linoleic acid zinc salt and cis-9, trans-11-conjugated linoleic acid zinc salt mixture: sodium fulvic acid: medical White oil: distilled water: glyceryl monostearate: butylated hydroxytoluene, the ratio is 35:25:20:19.18:0.8:0.02;
[0037]Heat 20 parts of medical white oil to 60°C, add trans-10, cis-12-conjugated linoleic acid zinc salt and cis-9, trans-11-conjugated linoleic acid zinc salt each 17.5 parts and anti- The oxidizing agent butylated 0.02 part of hydroxytoluene to obtain liquid A;
[0038] Add 25 parts of sodium fulvic acid into 19.18 parts of distilled water, stir to dissolve, and heat to 50°C to obtain liquid B;
[0039] Then add liquid B and 0.8 parts of surfactant glyceryl monostearate to liquid A, emulsify with a strong emulsifier for 2 hours, and cool to room temperature to obtain a compound containing zinc conjugated linoleic acid and humic acid Sodium medicinal oint...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 