5PB 7.5/4 pigment composition and entity colour block prepared by using same
A composition and pigment technology, applied in color measurement devices, color measurement using color charts, paper coatings, etc., can solve problems such as inability to accurately control, achieve strong practical value, good ratio reproducibility, weather resistance and stability high sex effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] Weigh 0.92 grams of PV23, 0.60 grams of PR101, 0.56 grams of PB15:3, and 1000 grams of CSC-B base material. Mix the above raw materials, and then apply the mixed composition evenly and evenly on the coated paper under the environmental conditions of relative humidity of 50%±5% and room temperature of 23±2°C. The wet film thickness of the coating is 250 μm, and then placed in a precision oven at 50±2°C for 3 to 4 hours to constant weight, taken out, cooled to room temperature, and obtained a physical color block.
Embodiment 2
[0024] Example 2: Weigh 0.91 grams of PV23, 0.59 grams of PR101, 0.55 grams of PB15:3, and 1000 grams of CSC-B base material. Manufacturing process is with embodiment 1.
Embodiment 3
[0025] Example 3: Weigh 0.93 grams of PV23, 0.60 grams of PR101, 0.57 grams of PB15:3, and 1005 grams of CSC-B base material. Manufacturing process is with embodiment 1.