Embodiment 1
[0011] Use sulfuric acid to adjust the pH value of the waste liquid to 0.9, then carry out pickling and tanning. Turn for 20 minutes; 0.5% sulfuric acid, add in three equal parts, each interval is 10 minutes, turn for 90 minutes; 0.2% fatliquor, turn for 30 minutes, stop for 2 hours; Aldehyde, 5.0% white tannin, turn for 3 hours, stop drum overnight.
Embodiment 2
[0013] Use sulfuric acid to adjust the pH value of the waste liquid to 1.2, and then carry out pickling tanning. The process is: 4% salt, 0.15% antifungal agent, turn for 10 minutes; 0.3% sulfuric acid, turn for 10 minutes; 70% waste liquid, turn for 10 minutes Minutes; 0.5% formic acid, turn for 20 minutes; 0.3% sulfuric acid, add three times in equal intervals, each interval of 10 minutes, turn for 90 minutes; stop for 2 hours; 60% waste liquid, warm up to 30 ° C, 1.0% glutaraldehyde, 5.0% White tannin, turn for 3 hours, stop drum overnight.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com