Elastic exterior wall paint and production method thereof
A technology of elastic exterior wall and production method, applied in the direction of biocide-containing paint, antifouling/underwater coating, coating, etc., can solve the problems of short retention time period, poor adhesion, poor stain resistance, etc., and achieve elasticity Long-lasting, good weather resistance, not easy to fade effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] An elastic exterior wall paint, prepared from the following components in parts by weight: 5 parts of dispersant, 1 part of wetting agent, 3 parts of defoamer, 1 part of multifunctional auxiliary agent, 10 parts of film-forming auxiliary agent, 20 parts of ethylene glycol, 4 parts of cellulose, 75 parts of kaolin, 150 parts of titanium dioxide, 175 parts of heavy calcium carbonate, 360 parts of elastic emulsion, 1.5 parts of preservative, 2 parts of thickener, 200 parts of deionized water.
[0030] The dispersant is sodium tripolyphosphate; the wetting agent is sulfonated oil; the defoamer is mineral oil; the multifunctional auxiliary agent is monomethylamine; the film-forming auxiliary agent is propylene glycol butyl ether ; The cellulose is methyl cellulose; the preservative is Dovi Hill-75; the thickener is polyacrylate.
[0031] The production method of elastic exterior wall paint described in the present embodiment comprises the following steps:
[0032] (1) Injec...
Embodiment 2
[0037] An elastic exterior wall paint is prepared from the following components in parts by weight: 2 parts of dispersant, 0.5 part of wetting agent, 1 part of defoamer, 0.5 part of multifunctional auxiliary agent, 6 parts of film-forming auxiliary agent, 15 parts of ethylene glycol, 2 parts of cellulose, 50 parts of kaolin, 130 parts of titanium dioxide, 100 parts of ground calcium carbonate, 300 parts of elastic emulsion, 1 part of preservative, 1 part of thickener, 150 parts of deionized water.
[0038] The dispersant is sodium tripolyphosphate; the wetting agent is sulfonated oil; the defoamer is mineral oil; the multifunctional auxiliary agent is water-based organic amine AMP-95; Propylene glycol butyl ether; The cellulose is methyl cellulose; The preservative is Dovihill-75; The thickener is polyacrylate.
[0039] The production method of elastic exterior wall paint described in the present embodiment is the same as embodiment 1.
Embodiment 3
[0041] An elastic exterior wall paint is prepared from the following components in parts by weight: 8 parts of dispersant, 1.5 parts of wetting agent, 5 parts of defoamer, 2 parts of multifunctional auxiliary agent, 12 parts of film-forming auxiliary agent, 30 parts of ethylene glycol, 7 parts of cellulose, 100 parts of kaolin, 180 parts of titanium dioxide, 200 parts of heavy calcium carbonate, 500 parts of elastic emulsion, 2 parts of preservative, 3 parts of thickener, 300 parts of deionized water.
[0042] The dispersant is sodium tripolyphosphate; the wetting agent is sulfonated oil; the defoamer is mineral oil; the multifunctional auxiliary agent is water-based organic amine AMP-95; Propylene glycol butyl ether; The cellulose is methyl cellulose; The preservative is Dovihill-75; The thickener is polyacrylate.
[0043] The production method of elastic exterior wall paint described in the present embodiment is the same as embodiment 1.