Embodiment 1
[0024] The raw ore is a primary platinum mine in Inner Mongolia, China.
[0025] (1) The raw ore is ground to -0.074mm, accounting for 80%, adding water to adjust the slurry to a pulp concentration of 27%, based on the weight of the ore, adding 2000g / t of sodium carbonate, stirring for 3 minutes, carboxymethyl cellulose 500g / t, Stir for 3 minutes, 240g / t butyl xanthate, stir for 2 minutes, 30g / t terpineol oil, stir for 1 minute, do rough selection; add 60g / t butyl xanthate, stir for 2 minutes, 10g / t terpineol oil, stir 1 minute, do a sweep; add 40g / t of butyl xanthate, stir for 2 minutes, pine oil 10g / t, stir for 1 minute, do a second sweep; add carboxymethyl cellulose 100g / t, stir for 3 minutes , carry out a beneficiation, add carboxymethyl cellulose 60g / t, stir for 3 minutes, carry out a second beneficiation, and obtain platinum group crude concentrate;
[0026] (2) Concentrate the platinum group rough concentrate to a slurry concentration of 45%, add water glass 100Kg / t ba...
Embodiment 2
[0029] The original ore is a primary platinum mine in a certain place in Heilongjiang, China.
[0030] (1) Grind the raw ore to -0.074mm to account for 75%, add water to adjust the pulp to a pulp concentration of 30%, add sodium carbonate 1000g / t, stir for 3 minutes, and water glass 2000g / t, stir for 3 minutes , 300g / t of butyl xanthate, stirred for 2 minutes, 30g / t of terpineol oil, stirred for 1 minute, and made rough selection; added 80g / t of butyl xanthate, stirred for 2 minutes, 10g / t of terpineol oil, stirred for 1 minute, Do a sweep; add 60g / t of butyl xanthate, stir for 2 minutes, 10g / t terpineol oil, stir for 1 minute, and do a second sweep; add 800g / t of water glass, stir for 3 minutes, and perform a sweep; Add 600g / t of water glass, stir for 3 minutes, and carry out second beneficiation; add 400g / t of water glass, stir for 3 minutes, and carry out three beneficiation to obtain coarse concentrate;
[0031] (2) Concentrate the rough concentrate to a pulp concentratio...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com