[0031] Carbonate powder, inorganic glue, and soluble organic gel are mixed evenly according to the ratio of 6.5:2:1.5, and the mixture is put into two semi-cylindrical molds and laid according to the requirements, and the temperature is kept at 45°C for 10 minutes, and the two semi-cylindrical molds are assembled into a cylinder placed on the pressurizing device of the core preparation device, under the condition of 35-40 °C, 10 MPa positive pressure for 20 minutes, and then removed after 10 minutes of back pressure, placed for 3-5 hours, dried at 40 °C, and the irregular end surface was cut off. Soak in 50°C distilled water for 20 minutes in a water bath, and then replace it with 50°C distilled water until the outflowing distilled water is clear, then the required core is obtained. The results are shown in the attached figure 1 shown.
Embodiment 2
[0034] Carbonate powder, inorganic glue, and soluble organic glue are mixed evenly according to 6:2:2, and the mixture is put into two semi-cylindrical molds and laid according to the requirements, and the temperature is kept at 45°C for 10 minutes, and the two semi-cylindrical molds are assembled into a cylindrical shape , placed on the pressurizing device of the core preparation device, under the condition of 35-40°C, 10MPa positive pressure for 20min, and back pressure for 10min, then take it off, place it for 3-5h, dry it at 40°C, cut off the irregular end face, and put it in a water bath Soak the pot with 50°C distilled water for 20 minutes, and then replace it with 50°C distilled water until the outflowing distilled water is clear, then the required core is obtained. The results are shown in the attached figure 2 shown.
[0035] This embodiment and figure 2 It shows that after increasing the proportion of soluble organic gel, the porosity of the core obtained increase...
Embodiment 3
[0037] Carbonate powder, inorganic glue, and soluble organic gel are mixed evenly according to the ratio of 6:2:2, and the mixture is filled into two semi-cylindrical molds and paved as required, and evenly spread on the surface of the substrate laid on one of the semi-cylindrical moulds. Place the selected proppant, pave it with soluble organic gel between the proppants, keep the temperature at 45°C for 10 minutes to make the raw materials in the two semi-cylindrical molds preliminarily cement and form, then assemble the two semi-cylindrical molds into a cylindrical shape, and place them on On the pressurizing device of the core preparation device, under the condition of 35-40°C, press 10MPa positive pressure for 20 minutes, take it off after 10 minutes of back pressure, place it for 3-5 hours, dry it at 40°C, cut off the irregular end face, and put it in a water bath Soak in distilled water at 50°C for 20 minutes, and then replace it with distilled water at 50°C until the out...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com