A transformer oil storage capsule
An oil storage capsule and transformer technology, applied in the field of electric power materials, can solve the problems of easy damage, short service life of the capsule, inconvenient production, etc., and achieve the effects of low cost, simple manufacturing process and easy realization.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] A transformer oil storage capsule, which is prepared according to the following method:
[0013] 1) Preparation of colloid: under normal temperature and pressure, 100 parts of polyvinyl chloride and 30 parts of polypropylene are mixed and mixed, and 3 parts of silicon carbide and 2 parts of aluminum oxide are added to the open mill. 1 part of sodium alginate, mixed evenly to form a colloid;
[0014] 3) Preparation of auxiliary materials: mix molybdenum disulfide, talc powder and barium sulfate according to the mass ratio of 2:1:1, and stir evenly to obtain the product;
[0015] 3) Preparation of adhesive plaster: Add ethyl acetate and auxiliary materials to the colloid in step 1), and stir evenly to form a glue; at 45°C and under normal pressure, put the glass fiber fabric on a glue spreader, and coat the above glue into a glue Adhesive plaster; dry it, and get it immediately; wherein, the mass ratio of colloid, ethyl acetate and auxiliary materials is 10:2:1.
[0016...
Embodiment 2
[0019] A transformer oil storage capsule, which is prepared according to the following method:
[0020] 1) Preparation of colloid: under normal temperature and pressure, 100 parts of polyvinyl chloride and 30 parts of polypropylene are mixed and mixed, and 3 parts of silicon carbide and 2 parts of aluminum oxide are added to the open mill. 1 part of sodium alginate, mixed evenly to form a colloid;
[0021] 3) Preparation of auxiliary materials: mix molybdenum disulfide, talc powder and barium sulfate according to the mass ratio of 2:1:1, and stir evenly to obtain the product;
[0022] 3) Preparation of adhesive plaster: Add ethyl acetate and auxiliary materials to the colloid in step 1), and stir evenly to form a glue; at 45°C and under normal pressure, put the glass fiber fabric on a glue spreader, and coat the above glue into a glue Adhesive plaster; dry it, and get it immediately; wherein, the mass ratio of colloid, ethyl acetate and auxiliary materials is 20:3:2.
[0023...