A kind of red mud soil matrix and preparation method thereof
A technology for red mud and soil is applied in the field of red mud soil matrix and its preparation, and can solve the problems of fugitive dust polluting the air, poor air permeability, complicated process and the like
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0045] The application provides a preparation method of red mud soil matrix, such as figure 1 shown, including the following steps:
[0046] Step S1, using a crusher to crush the biomass raw material into biomass powder;
[0047] Step S2, transporting biomass powder, water and catalyst into a stirring tank for stirring to obtain a mixture;
[0048] Step S3, adding the mixture to the autoclave at a speed of V 1 The autoclave is heated up to T 1 After that, keep it warm for 5-20 hours; then cool to room temperature to obtain the hydrothermal carbonization product;
[0049] Step S4, performing solid-liquid separation on part of the hydrothermal carbonization products to obtain hydrothermal charcoal and hydrothermal charcoal liquid; the remaining hydrothermal carbonization products are set aside;
[0050] Step S5, carbonizing the hydrothermal charcoal to obtain modified hydrothermal charcoal;
[0051] Step S6, mix the modified hydrothermal charcoal, the remaining hydrothermal...
Embodiment 1
[0098] The preparation method of the red mud soil matrix of the present embodiment may further comprise the steps:
[0099] Step S1, adding the biomass raw material (in this embodiment, straw) into the crusher 1, and the crusher 1 crushes the straw into a powder with a particle size of 1 mm;
[0100] Step S2, use the material lifting mechanism 4 to transport the powder into the mixing tank 2 from the first feeding port, and then add water and catalyst (the catalyst is red mud in this embodiment) into the mixing tank 2 through the second feeding port , stirring to obtain a mixture, the stirring speed is 500rpm, the stirring time is 10min, and the mass ratio of powder, water and catalyst is: 0.05:1:0.0025;
[0101] Step S3, adding the mixture to the autoclave 3, heating the autoclave 3 at 200°C / h, and keeping the temperature at 200°C for 20 hours; then cooling to room temperature to obtain a hydrothermal carbonization product; wherein, the mixture Volume is 1 / 3 of the volume of...
Embodiment 2
[0107] The preparation method of the red mud soil matrix of the present embodiment may further comprise the steps:
[0108] Step S1, adding the biomass raw material (fallen leaves in this embodiment) into the crusher 1, and the crusher 1 crushes the fallen leaves into a powder with a particle size of 3mm;
[0109] Step S2, use the material lifting mechanism 4 to transport the powder into the stirring tank 2 from the first feeding port, and then add water and catalyst (the catalyst is potassium carbonate in this embodiment) into the stirring tank 2 through the second feeding port , stirring to obtain a mixture, the stirring speed is 200rpm, the stirring time is 30min, and the mass ratio of powder, water and catalyst is: 0.2:1:0.01;
[0110] Step S3, adding the mixture to the autoclave 3, heating the autoclave 3 at 150°C / h, and keeping the temperature at 380°C for 10 hours; then cooling to room temperature to obtain a hydrothermal carbonization product; wherein, the mixture Vol...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com