Embodiment 1
[0028] Step 1. The moisture content of the shredded tobacco leaves of the Huangshan A brand sheet drying group is 18.50%, and the temperature and humidity are not increased by using a tunnel-type temperature-increasing and humidifying machine. The material flow rate of the shredded tobacco before entering the thin plate shred dryer is 3500kg / h, and the moisture content of the output after the thin plate is dried is 12.82%. Calculate the dehydration amount M of the drying process 1 It is 228.0kg / h.
[0029] Step 2. Adjust the wind balance of the thin plate dryer so that the feed end of the thin plate dryer is adjusted to a slight negative pressure of 0~-20 micropascals, and the discharge end is adjusted to a negative pressure of -5~-20 micropascals. Measuring holes are set on the air inlet duct of the horizontal section in front of the thin plate wire drying machine, as the hot air wind speed detection point;
[0030] Measure the pipe diameter r of the air inlet pipe as 400mm...
Embodiment 2
[0035] Step 1. The moisture content of cut tobacco leaves of Huangshan A brand sheet drying group is 18.50% after being cut into shreds, and the moisture content of shredded tobacco is 22.46% after being heated and humidified by a tunnel-type warming and humidifying machine. The material flow rate of shredded tobacco before entering the sheet drying machine is 5000kg / h, the moisture content of the output after the thin plate is dried is 12.35%. Calculate the dehydration amount M of the drying process 1 It is 576.7kg / h.
[0036] Step 2. Adjust the wind balance of the thin plate dryer so that the feed end of the thin plate dryer is adjusted to a slight negative pressure of 0~-20 micropascals, and the discharge end is adjusted to a negative pressure of -5~-20 micropascals. Measuring holes are set on the air inlet duct of the horizontal section in front of the thin plate wire drying machine, as the hot air wind speed detection point;
PUM
| Property | Measurement | Unit |
|---|---|---|
| dehydration rate | aaaaa | aaaaa |
| dehydration rate | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com