An ecological revetment and affinity technology, applied in environmental engineering and fields, can solve problems such as unsatisfactory river regulation and bank slope protection, adverse effects on the ecological environment, limited pebble storage, etc., to achieve response efficiency, reduce adverse effects, The effect of protecting the environment
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0036]An ecological revetment material with good biological affinity, comprising the following raw materials and their weight percentages: 30%-40% of cement, 10%-16% of water, 9%-15% of granite powder, fly ash 8%-12% for gravel, 7%-10% for gravel, 3%-7% for binder, 4%-5% for water reducing agent, 3%-5% for cullet, 2.5% for concrete activator %-5%, photocatalytic material 1%-4%, concrete reinforcing fiber 1.5%-4%, concrete air-entraining agent 1%-2%.
[0037] Made of raw materials with the following mass percentages: 32% of cement, 14% of water, 14% of granite dust, 10% of fly ash, 9% of gravel, 4% of binder, and 4% of water reducer %, broken glass is 4%, concrete activator is 3%, photocatalytic material is 3%, concrete reinforcing fiber is 2%, concrete air-entraining agent is 1%.
[0038] A preparation method of an ecological revetment material with good bio-affinity, comprising the following steps:
[0039] a. First crush the granite powder and cullet, and screen the granit...
Embodiment 2
[0047] An ecological revetment material with good biological affinity, including the following raw materials and their weight percentages: 30% cement, 10% water, 10% granite dust, 10% fly ash, 9% gravel, 7% for binder, 4% for water reducer, 5% for cullet, 5% for concrete activator, 4% for photocatalytic material, 4% for concrete reinforcing fiber, and 2% for concrete air-entraining agent %, its production process is the same as the operation steps of Example 1. This example increases the tensile strength of the concrete cube by increasing the binder content, and avoids separation under its own gravity and external force.
Embodiment 3
[0049] An ecological revetment material with good biological affinity, including the following raw materials and their weight percentages: 40% cement, 14% water, 9% granite dust, 8% fly ash, 7% gravel, 3% for binder, 5% for water reducing agent, 3% for cullet, 5% for concrete activator, 1% for photocatalytic material, 3% for concrete reinforcing fiber, 2% for concrete air-entraining agent %, the production process of this embodiment is the same as the operation steps of Embodiment 1. In this embodiment, the overall bonding strength of the concrete cube is improved by increasing the cement content, and it can also effectively resist water body erosion and meet the needs of ecological revetment.