Embodiment 1
[0041] A kind of preparation method of green environment-friendly slow-release oxygenation agent, its technological process is as follows:
[0042] Step 1: Pour 10 mL of absolute ethanol into a container containing 0.2 g of ozokerite under the condition of heating in a water bath at 60°C, and stir until the ozokerite is completely dissolved to prepare an embedding agent solution with a mass-volume ratio of 0.02 g / mL , i.e. ozokerite-ethanol mixture;
[0043] Step 2, take by weighing 7.0g calcium peroxide, 2.8g bentonite respectively, stir and mix with calcium peroxide after bentonite passes 200 mesh sieves, make oxygenate mixture;
[0044] Step 3, adding the embedding agent solution prepared in step 1 to the oxygenate mixture prepared in step 2, and stirring evenly to obtain the oxygenate embedding mixture;
[0045] Step 4: Compress the oxygenate embedding mixture prepared in step 3 into tablets, heat in an oven at 50±5°C for 2 to 3 hours to completely volatilize the absolute...
Embodiment 2
[0047] A kind of preparation method of green environment-friendly slow-release oxygenation agent, its technological process is as follows:
[0048] Step 1: Pour 10 mL of absolute ethanol into a container containing 0.4 g of ozokerite under the condition of heating in a water bath at 60°C, and stir until the ozokerite is completely dissolved to prepare an embedding agent solution with a mass-volume ratio of 0.04 g / mL , i.e. ozokerite-ethanol mixture;
[0049] Step 2, take by weighing 7.0g calcium peroxide, 2.6g bentonite respectively, stir and mix with calcium peroxide after bentonite crosses 200 mesh sieves, make oxygenator mixture;
[0050] Step 3, adding the embedding agent solution prepared in step 1 to the oxygenate mixture prepared in step 2, and stirring evenly to obtain the oxygenate embedding mixture;
[0051] Step 4: Compress the oxygenate embedding mixture prepared in step 3 into tablets, heat in an oven at 50±5°C for 2 to 3 hours to completely volatilize the absolu...
Embodiment 3
[0053] A kind of preparation method of green environment-friendly slow-release oxygenation agent, its technological process is as follows:
[0054] Step 1, at room temperature, pour 5 mL of ether into a container containing 0.5 g of palm wax, stir until the palm wax is completely dissolved, and prepare an embedding agent solution with a mass-volume ratio of 0.1 g / mL, namely stearic acid - Ether mixture;
[0055] Step 2, take by weighing 8.0g calcium peroxide, 1.5g kaolin respectively, kaolin passes through 100 mesh sieves and stirs and mixes with calcium peroxide evenly, makes oxygenator mixture;
[0056] Step 3, adding the embedding agent solution prepared in step 1 to the oxygenate mixture prepared in step 2, and stirring evenly to obtain the oxygenate embedding mixture;
[0057] Step 4, compress the embedding mixture of oxygenate prepared in step 3 into a tablet, and put it in a fume hood until the ether is completely volatilized to obtain the slow-release oxygenate.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com