Woolen yarn waterproof oil preventing treating tech.
A treatment process, waterproof and oil-proof technology, applied in liquid/gas/steam yarn/filament treatment, other chemical processes, chemical instruments and methods, etc. Good oil performance and other problems, to achieve the effect of less dosage and uniform waterproof and oil-proof performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] Wool waterproof and oil-proof treatment process, it comprises the following steps:
[0014] (1) Put the velvet in the dye tank of the skein dyeing machine, add 30 parts by weight of water to 1 part by weight of the velvet, add water to the dye trough of the skein dyeing machine and immerse the velvet in the liquid, according to the weight of the water Add 2% of the nanometer water and oil repellent to the dyeing tank of the skein dyeing machine, and then start the turning wheel of the skein dyeing machine, so that the liquid in the dyeing tank starts to circulate, and the wool is soaked in the liquid for 40 minutes. then remove;
[0015] (2) The product obtained in step (1) is placed in a spin-drying device for 8 minutes of spin-drying and dehydration;
[0016] (3) Put the product obtained in step (2) into a skein dryer and dry it for 40 minutes at a drying temperature of 90°C.
[0017] The fleece with waterproof and oil-proof properties can be obtained through the ab...
Embodiment 2
[0019] Wool waterproof and oil-proof treatment process, it comprises the following steps:
[0020] (1) Put the velvet in the dyeing tank of the skein dyeing machine, add 25 parts by weight of water to the skein dyeing machine according to 1 weight part of the velvet, add water to the dyeing tank of the skein dyeing machine and soak the velvet in the liquid, and add water according to the weight of the water Add 1% of the nanometer waterproof and oil-repellent agent into the dyeing tank of the skein dyeing machine, and then start the turning wheel of the skein dyeing machine, so that the liquid in the dyeing tank starts to circulate, and the wool is soaked in the liquid for 50 minutes. then remove;
[0021] (2) The product obtained in step (1) is placed in a spin-drying device for 5 minutes of spin-drying and dehydration;
[0022] (3) Put the product obtained in step (2) into a skein dryer and dry it for 50 minutes at a drying temperature of 85°C.
[0023] The fleece with wat...
Embodiment 3
[0025] It includes the following steps:
[0026] (1) Put the velvet in the dye tank of the skein dyeing machine, add 35 parts by weight of water to 1 part by weight of the velvet, add water to the dye trough of the skein dyeing machine and soak the velvet in the liquid, according to the weight of the water Add nanometer waterproof and oil-repellent agent into the dyeing tank of the skein dyeing machine, and then start the turning wheel of the skein dyeing machine, so that the liquid in the dyeing tank starts to circulate, and the wool is soaked in the liquid for 30 minutes. then remove;
[0027] (2) The product obtained in step (1) is placed in a spin-drying device for 10 minutes of spin-drying and dehydration;
[0028] (3) Put the product obtained in step (2) into a skein dryer and dry it for 30 minutes at a drying temperature of 100°C.
[0029] The fleece with waterproof and oil-proof properties can be obtained through the above process.