A nano-composite, rubber material technology, applied in the field of rubber materials, can solve the problems of limited promotion prospects, secondary electromagnetic pollution, less absorption, etc., and achieve the effect of improving working and living environment, promoting upgrading, and high absorption rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0071] The nanocomposite wave-absorbing natural rubber material contains 90-120 parts of rubber; 1-6 parts of diethylpropylbenzene peroxide; 1-4 parts of triallyl isocyanurate; 2-5 parts of zinc powder; 1-3 parts Styrene-acrylonitrile copolymer; 1-2 parts of N.RD anti-aging agent; 0.5-1.5 parts of N.MB anti-aging agent; 30-40 parts of silicon dioxide or carbon black; 6-12 parts of dioctyl sebacate ester; 0.6-1.2 parts of polyvinyl fluoride; 8-40 parts of nano-β-silicon carbide; 1-6 parts of nano-nickel powder; 8-22 parts of polyaniline.
[0072] The preparation method of product is carried out according to the following steps:
[0073] a. Take the required weight of the rubber body according to the proportion ratio for later use, and take the required weight for the additive according to the proportion ratio for later use;
[0074] b. Preparation of nano-masterbatch: Weigh the required weight of nano-β-silicon carbide, nano-nickel powder, and liquid polyaniline according to t...
Embodiment 2
[0081] The nanocomposite wave-absorbing natural rubber material contains 90 parts of rubber; 6.0 parts of diethylpropylbenzene peroxide; 4.0 parts of triallyl isocyanurate; 5.0 parts of zinc powder; 3.0 parts of styrene-acrylonitrile copolymer; 2.0 parts N.RD anti-aging agent; 1.5 parts of N.MB anti-aging agent; 40.0 parts of silicon dioxide or carbon black; 12.0 parts of dioctyl sebacate; 1.2 parts of polyvinyl fluoride; 40.0 parts of nano-β-silicon carbide; 6.0 parts Nano nickel powder; 22.0 parts of polyaniline. The preparation method of product is with embodiment 1.
Embodiment 3
[0083] The nanocomposite wave-absorbing natural rubber material contains 100 parts of rubber; 5.0 parts of diethylpropylbenzene peroxide; 3.0 parts of triallyl isocyanurate; 4.0 parts of zinc powder; 2.0 parts of styrene-acrylonitrile copolymer; 2.0 parts N.RD anti-aging agent; 1.0 parts of N.MB anti-aging agent; 38.0 parts of silicon dioxide or carbon black; 10.0 parts of dioctyl sebacate; 1.0 parts of polyvinyl fluoride; 30.0 parts of nano-β-silicon carbide; 5.0 parts Nano nickel powder; 18.0 parts of polyaniline. The preparation method of product is with embodiment 1.