[0009] A gloss treatment method for electrostatic flocking fluff, the process steps are as follows:
[0010] 1): Use 10%-30% titanium dioxide (TiO 2 ) And 70%~90% water glass (Na 2 SiO 3 ) After mixing, stir at high speed for 20-40 minutes to fully dissolve;
[0011] In this process, it is best to use 20% titanium dioxide (TiO2) and 80% water glass (Na2SiO3) to stir for 30 minutes at a stirring speed of 1200 revolutions per minute until they are fully dissolved.
[0012] 2): 3-8% of the solution obtained in step (1) is added when the electrostatic flocking hair is subjected to electrical properties treatment, preferably 5% of the solution obtained in step (1) is added.
[0013] Because this product adds titanium dioxide (TiO 2 ) And water glass (Na 2 SiO 3 ), using water glass (Na 2 SiO 3 ) The mediating effect of the adhesion to the fiber will make the titanium dioxide (TiO 2 ) Is attached to the surface of the fluff, so as to effectively change the gloss of the electrostatic flo...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com