Method for enhancing inner protection film hydrophilicity of polaroid
A technology of protective film and polarizer, applied in polarizing elements and other directions, can solve problems such as increased production cost, and achieve the effects of reducing the pressure of environmental protection treatment, improving the degree of infiltration, and reducing the concentration
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment
[0067] Material Description:
[0068] Polarizer inner protective film: Triacetyl cellulose film (abbreviated as TAC film, the same below), produced by LOFO company in Germany;
[0069] Alkali: NaOH, commercially available, chemically pure;
[0070] Surfactant A: dodecyltrimethylammonium chloride, commercially available, chemically pure;
[0071] Surfactant B: cetyltrimethylammonium bromide, commercially available, chemically pure;
[0072] PVA (polyvinyl alcohol) film, product of Japan Kuraray Company, VF-P;
[0073] Adhesive: PVA aqueous solution (PVA-124: product of Kuraray Co.), concentration 5% (weight ratio).
[0074] Hydrophilic effect test:
[0075] Testing instrument: SL200A dynamic / static contact angle meter.
[0076] Detection method: In the environment of 25±1℃ / 60±5%RH, drop pure water on the surface of the film to be tested, and read the contact angle θ within 10 seconds (see Image 6 , D is the film to be tested). 5 points were measured for each sample, and...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com