Facial line for door sleeve and processing method thereof
A face line and main face technology, which is applied in the field of door cover face line and its processing, can solve the problems of high cost and poor bonding strength, and achieve the effects of easy repair, consistent texture and cost reduction
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] As shown in the figure, it includes a main face line 10, a tenon board 20, and a side board 3. The upper end of the tenon board 20 is provided with a slope 21, and the upper end of the side board 30 is provided with a slope 31; The slope 11 with the slope 11 corresponding to the slope 21,31 of the side plate 30 and itself, the step 11 is made up of the slope 12 and the bottom surface 13; The slope 12 is combined, the tenon plate 20 and the side plate 30 are combined with the bottom surface 13 of the two steps 11 respectively, and the tenon plate 20, the side plate 30 and the main face line 10 are combined to form two on the main face line 10. Two sides are provided with chamfering 41. The surfaces of the main face line 10 , tenon board 20 and side board 30 are impregnated paper veneer 50 . After the tenon plate 20 , the side plate 30 and the main face line 10 are combined, the chamfer 41 provided on the two sides formed above the main face line 10 is a thermal transfer...
Embodiment 2
[0031] There is a square groove 71 in the middle of the U-shaped mold 70, and the two inner corners at the bottom of the square groove 71 are respectively provided with grooves 72, and the left and right sides of the square groove 71 are respectively provided with steps 73, and each group of square columns 90 is placed in two U-shaped molds 70, the surfaces of the two thin plates 80 correspond to the bottom surfaces of the square grooves 71 of the two U-shaped molds 70, and two main face lines 10 are placed on the surfaces corresponding to the four steps 73. The stripping plate 74, the thickness of the stripping plate 74 is greater than the depth of the step 73, so that the glue extruded from the four sides will not affect the demoulding; other structures and methods are the same as in Embodiment 1.
Embodiment 3
[0033] The surfaces of the main face line 10 , tenon plate 20 and side plate 30 are veneers, and the veneer is coated with a paint coating; other structures and methods are the same as in Embodiment 1.
PUM
Login to View More Abstract
Description
Claims
Application Information