Tulobuterol-containing aquogel patch and preparation method thereof
A technology of hydrogel patch and cross-linking agent, which is applied in the field of hydrogel patch containing tulobuterol and its preparation, and can solve the problems of hydrogel matrix hardening, viscosity decrease, cohesion instability, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0053] The preparation method of hydrogel patch of the present invention, comprises the steps:
[0054] Mix appropriate amount of polymer framework material, crosslinking agent and humectant evenly to obtain phase I;
[0055] Disperse the cross-linking regulator and tulobuterol composed of two or more organic acids in an appropriate amount of distilled water to obtain phase II;
[0056] Mix Phase II and Phase I, stir evenly and then coat.
[0057] Among the two or more organic acids constituting the crosslinking regulator, at least one organic acid is selected from tartaric acid, and at least another organic acid is selected from citric acid, gluconic acid, lactic acid, malic acid, and hydroxysuccinic acid.
[0058] Preferably, phase I also contains fillers and skin penetration enhancers.
[0059] Preferably, the phase II also contains a tackifier, and the tackifier is a methyl vinyl ether / maleic anhydride copolymer.
Embodiment 1
[0061] Embodiment 1 (making 100 tablets of cataplasm altogether)
[0062] Tulobuterol 10g
[0063] Polyacrylic acid / sodium polyacrylate copolymer NP-600 155g
[0064] Methyl vinyl ether / maleic anhydride copolymer 20g
[0065] Polyvinylpyrrolidone K90 10g
[0066] Aluminum hydroxide 2.5g
[0067] Aluminum glycylate 2.5g
[0068] Citric acid 2g
[0069] Tartaric acid 2g
[0070] Glycerin 650g
[0071] Azone 8g
[0072] Distilled water 1400g
[0073] Preparation method: first crush each matrix raw material to a certain fineness, weigh it precisely according to the prescription ratio, and carry out batching, mix polyacrylic acid / sodium polyacrylate copolymer NP-600, aluminum hydroxide, aluminum glycolate, azone, and glycerin Uniformly used as phase I, citric acid, tartaric acid, tulobuterol, methyl vinyl ether / maleic anhydride copolymer, distilled water as phase II were fully dispersed and heated until clear, then phase II was quickly added to phase I and mixed evenly, S...
Embodiment 2
[0075] Embodiment 2 (100 pieces of cataplasms prepared in total)
[0076] Tulobuterol 8g
[0077] Polyacrylic acid / sodium polyacrylate copolymer NP900 125g
[0078] Methyl vinyl ether / maleic anhydride copolymer 16g
[0079] Methylcellulose 2.6g
[0081] Aluminum glycylate 2g
[0082] Lactic acid 2.5g
[0083] Tartaric acid 3.5g
[0084] Butanediol 800g
[0085] N-Methylpyrrolidone 10g
[0086] Distilled water 1700g
[0087]The preparation method is the same as in Example 1. The prepared hydrogel patch has good physical properties, the appearance is flat and bright, and the viscosity meets the requirements. The crosslinking time is controlled within 2-4 hours, and the appearance, viscosity, cohesion, etc. have no obvious changes after storage for 6 months. , indicating good stability.
PUM
Property | Measurement | Unit |
---|---|---|
Holding power | aaaaa | aaaaa |
Initial tack | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com