Method for continuously and rapidly adjusting width decrease of mold in online manner
A rapid adjustment and crystallizer technology, which is applied in the field of online width adjustment of continuous casting molds, can solve the problems of affecting the production rhythm of steel mills, increasing production costs, and reducing slab output, so as to improve production quality, increase work efficiency, Effect of Reducing Wedge Blank Waste
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0049] The taper on one side of the crystallizer is 9mm, the taper reduction during the width adjustment process is 30mm, and the width adjustment acceleration is set to 20mm / min 2 , the casting speed is 1.0m / min, the height of the mold is 900mm, the height of the meniscus is 800mm, the time for molten steel to go from the meniscus to the outlet of the mold is 0.8min, the width of both sides is adjusted, and the width is reduced by 400mm, and the corresponding The relationship between speed, time and length of wedge segment during widening process.
[0050] From the above analysis, it can be seen that if the width is adjusted on both sides of the crystallizer, the width of the single side adjustment is 200mm, that is, L=200mm. Correspondingly, ΔT=30mm, a=20mm / min 2 , t 0 =0.8min, V c =1.0m / min=1000mm / min. Therefore, the control parameters are:
[0051] 1. Cone adjustment time t 1 :
[0052] t 1 = ΔT ...
Embodiment 2
[0063] The taper on one side of the crystallizer is 6mm, the taper reduction during the width adjustment process is 15mm, and the width adjustment acceleration is set to 15mm / min 2 , the casting speed is 1.0m / min, the height of the mold is 900mm, the height of the meniscus is 800mm, the time for molten steel to go from the meniscus to the outlet of the mold is 0.8min, the width of both sides is adjusted, and the width is reduced by 200mm, and the corresponding The relationship between speed, time and length of wedge segment during widening process.
[0064] From the above analysis, it can be seen that if the width is adjusted on both sides of the crystallizer, the width of the single side adjustment is 100mm, that is, L=100mm. Correspondingly, ΔT=15mm, a=15mm / min 2 , t 0 =0.8min, V c =1.0m / min=1000mm / min. Therefore, the control parameters are:
[0065] 1. Cone adjustment time t 1 :
[0066] t 1 = ΔT ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com