Formula and synthesis process of novel block hydrophilic silicone oil
A hydrophilic silicone oil, a new type of technology, applied in textiles, papermaking, fiber processing, etc., can solve the problems of complex procedures, the inability of amino silicone oil to be used directly, and the generation of silicone oil spots, and achieve the effect of simple production process.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0011] In the first step, 45 parts of aliphatic polyether diamine, 340 parts of isopropanol, and 400 parts of epoxy-terminated silicone oil are put into In the reaction kettle, heat up to 80°C and keep warm for 8 hours; in the second step, add 6 parts of sulfuric acid solution with a concentration of 20%, and balance the reaction for 30 minutes; in the third step, add 450 parts of dipropylene glycol, balance the reaction for 30 minutes, negative Press and evacuate, heat up to 100°C, pump to the highest degree of vacuum, exhaust the volatile isopropanol, balance the reaction for 30 minutes, and cool down to 50°C; the fourth step, add 170 parts of isomeric alcohol polyoxyethylene ether and 3 parts Glacial acetic acid, stir evenly, cool down to 35°C, and discharge.
Embodiment 2
[0013] In the first step, 35 parts of aliphatic polyether diamine, 300 parts of isopropanol, and 360 parts of epoxy-terminated silicone oil are put into In the reaction kettle, heat up to 80°C, and keep it warm for 8 hours; in the second step, add 4 parts of sulfuric acid solution with a concentration of 20%, and balance the reaction for 30 minutes; in the third step, add 400 parts of dipropylene glycol, balance the reaction for 30 minutes, negative Press and evacuate, raise the temperature to 100°C, and pump to the highest degree of vacuum, exhaust the volatile isopropanol, balance the reaction for 30 minutes, and cool down to 50°C; the fourth step, add 150 parts of isomeric alcohol polyoxyethylene ether and 1 part Glacial acetic acid, stir evenly, cool down to 35°C, and discharge.
Embodiment 3
[0015] In the first step, 40 parts of aliphatic polyether diamine, 320 parts of isopropanol, and 380 parts of epoxy-terminated silicone oil are put into In the reaction kettle, heat up to 80°C, and keep it warm for 8 hours; in the second step, add 5 parts of sulfuric acid solution with a concentration of 20%, and balance the reaction for 30 minutes; in the third step, add 420 parts of dipropylene glycol, balance the reaction for 30 minutes, negative Press and vacuum, heat up to 100°C, pump to the highest degree of vacuum, exhaust the volatile isopropanol, balance the reaction for 30 minutes, cool down to 50°C; the fourth step, add 160 parts of isomeric alcohol polyoxyethylene ether and 2 parts Glacial acetic acid, stir evenly, cool down to 35°C, and discharge.