A technology of glass-ceramics and rare-earth ions, which is applied in rare-earth-ion-doped Cs2LiLuCl6 glass-ceramics and its preparation field, can solve problems such as difficulty in growing large-sized crystals, affecting practical applications, and poor mechanical properties, and achieves low production costs, Improved efficiency and good mechanical properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] Embodiment 1: Table 1 shows the glass formula and the first crystallization temperature value of Embodiment 1.
[0023] Table 1
[0024]
[0025] The specific preparation process is as follows: the first step, Cs 2 Li Lu 0.95 Ce 0.05 Cl 6 Raw materials are CsCl, LiCl, LuCl 3 , CeCl 3 Mix and sinter, weigh 50 grams of analytically pure raw materials according to the formula in Table 1, add 2.5 grams of NH 4 HF 2 , 2.5 g NH 4 HCl 2 , Mix the raw materials evenly and pour them into a quartz crucible to melt, the melting temperature is 1350 ° C, keep warm for 2 hours, pour the glass melt into a cast iron mold, then place it in a muffle furnace for annealing, and keep it warm at the glass transition temperature Tg for 1 Hours later, cool down to 50°C at a rate of 10°C / hour, turn off the power supply of the muffle furnace to automatically cool down to room temperature, and take out the glass; in the second step, according to the experimental data of thermal analys...
Embodiment 2
[0027] Embodiment 2: Table 2 shows the glass formula and the first crystallization temperature value of Embodiment 2.
[0028] Table 2
[0029]
[0030] The specific preparation process is as follows: the first step, Cs 2 Li Lu 0.8 Eu 0.2 Cl 6 Raw materials are CsCl, LiCl, LuCl 3 , EuCl 3 Mix and sinter, weigh 50 grams of analytically pure raw materials according to the formula in Table 2, add 2.5 grams of NH 4 HF 2 , 2.5 g NH 4 HCl 2 , mix the raw materials evenly and pour them into a corundum crucible for melting, the melting temperature is 1400°C, keep warm for 1 hour, pour the glass melt into a cast iron mold, then place it in a muffle furnace for annealing, and keep warm at the glass transition temperature Tg for 1 hour Hours later, cool down to 50°C at a rate of 10°C / hour, turn off the power supply of the muffle furnace to automatically cool down to room temperature, and take out the glass; in the second step, according to the experimental data of thermal ana...
Embodiment 3
[0032] Embodiment 3: Table 3 shows the glass formula and the first crystallization temperature value of Embodiment 3.
[0033] table 3
[0034]
[0035] The specific preparation process is as follows: the first step, Cs 2 Li Lu 0.9 Tb 0.1 Cl 6 Raw materials are CsCl, LiCl, LuCl 3 , TbCl 3 Mix and sinter, weigh 50 grams of analytically pure raw materials according to the formula in Table 3, add 2.5 grams of NH 4 HF 2 , 2.5 grams of NH4HCl 2 , Mix the raw materials evenly and pour them into a quartz crucible to melt, the melting temperature is 1450°C, keep warm for 1.5 hours, pour the glass melt into a cast iron mold, then place it in a muffle furnace for annealing, and keep warm at the glass transition temperature Tg for 1 hour Hours later, the temperature was lowered to 50° C. at a rate of 10° C. / hour, the power of the muffle furnace was turned off and the temperature was automatically lowered to room temperature, and the glass was taken out. In the second step, ac...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com