Examples
Embodiment 1
[0048] Such as figure 1 Shown, the manufacture method of a kind of poplar summer mat of the present embodiment, comprises the steps:
[0049] (1) Make poplar strips
[0050] Select poplar trees that are at least five years old, and after removing the bark, cut them into poplar strips by woodworking machinery;
[0051] (2) Pressure cooking
[0052] The obtained poplar strips were pressure-cooked in a cooking pot, the cooking pressure was 0.02MPa, and the cooking time was 9h; then, it was taken out and left to stand for 5h before it was subjected to pressure cooking for the second time, and the second pressure cooking The cooking pressure is 0.01MPa, and the cooking time is 7h; the poplar strips are taken out from the cooking pot after the second cooking;
[0053] (3) dry
[0054] Drying the poplar strips that have completed secondary pressure cooking to a water content of 6%;
[0055] (4) Grinding and polishing
[0056] The dried poplar strips are passed through a grinder...
Embodiment 2
[0070] Such as figure 1 Shown, the manufacture method of a kind of poplar summer mat of the present embodiment, comprises the steps:
[0071] (1) Make poplar strips
[0072]Select poplar trees that are at least five years old, and after removing the bark, cut them into poplar strips by woodworking machinery;
[0073] (2) Pressure cooking
[0074] The obtained poplar strips were pressure-cooked in a cooking pot, the cooking pressure was 0.03 MPa, and the cooking time was 11 hours; then, they were taken out and left to stand for 6 hours, and then pressure-cooked for the second time, the second pressure-cooking The cooking pressure is 0.02MPa, and the cooking time is 8h; the poplar strips are taken out from the cooking pot after the second cooking;
[0075] (3) dry
[0076] Drying the poplar strips that have completed secondary pressure cooking to a water content of 7%;
[0077] (4) Grinding and polishing
[0078] The dried poplar strips are passed through a grinder and a p...
Embodiment 3
[0092] Such as figure 1 Shown, the manufacture method of a kind of poplar summer mat of the present embodiment, comprises the steps:
[0093] (1) Make poplar strips
[0094] Select poplar trees that are at least five years old, and after removing the bark, cut them into poplar strips by woodworking machinery;
[0095] (2) Pressure cooking
[0096] The obtained poplar strips were pressure-cooked in a cooking pot, the cooking pressure was 0.025MPa, and the cooking time was 10h; then, it was taken out and left to stand for 5.5h before it was subjected to pressure cooking for the second time. The cooking pressure of cooking is 0.015MPa, and the cooking time is 7.5h; after the second cooking, poplar strips are taken out from the cooking pot;
[0097] (3) dry
[0098] Drying the poplar strips that have completed secondary pressure cooking to a water content of 6.5%;
[0099] (4) Grinding and polishing
[0100] The dried poplar strips are passed through a grinder and a polishin...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com