[0021] A surface treatment method for a plastic chair, comprising the following steps:
[0022] S1, annealing the plastic chair;
[0023] S2, degreasing the annealed plastic chair;
[0024] S3, de-staticize and de-dust the degreasing-treated plastic chairs;
[0025] S4, treating the surface of the plastic chair treated in step 3 so that its surface flatness is 0.5mm;
[0026] S5, spray primer on the surface of the plastic chair, then dry;
[0027] S6, then spray the topcoat again, after the topcoat is naturally leveled on the surface, then spray the topcoat;
[0028] S7, then dry and cure the plastic chair at a temperature of 60°C for 8 minutes, and then dry at a temperature of 30°C until the moisture content is 4%.
[0029] In the step 1, the plastic chair is heated to 50°C and kept for 1.5h.
[0030] In said step 2, clean the plastic chair with gasoline or alcohol, then rinse its surface with pure water, and finally dry it at room temperature.
[0031] In described ste...
Embodiment 2
[0035] A surface treatment method for a plastic chair, comprising the following steps:
[0036] S1, annealing the plastic chair;
[0037] S2, degreasing the annealed plastic chair;
[0038] S3, de-staticize and de-dust the degreasing-treated plastic chairs;
[0039] S4, treating the surface of the plastic chair treated in step 3, so that its surface flatness is 1.5mm;
[0040] S5, spray primer on the surface of the plastic chair, then dry;
[0041] S6, then spray the topcoat again, after the topcoat is naturally leveled on the surface, then spray the topcoat;
[0042] S7, then dry and cure the plastic chair at a temperature of 80°C for 10 minutes, and then dry at a temperature of 50°C until the moisture content is 6%.
[0043] In the step 1, the plastic chair is heated to 70° C. and kept for 3 hours.
[0044] In said step 2, clean the plastic chair with gasoline or alcohol, then rinse its surface with pure water, and finally dry it at room temperature.
[0045] In descri...
Embodiment 3
[0049] A surface treatment method for a plastic chair, comprising the following steps:
[0050] S1, annealing the plastic chair;
[0051] S2, degreasing the annealed plastic chair;
[0052] S3, de-staticize and de-dust the degreasing-treated plastic chairs;
[0053] S4, treating the surface of the plastic chair treated in step 3 so that its surface flatness is 1 mm;
[0054] S5, spray primer on the surface of the plastic chair, then dry;
[0055] S6, then spray the topcoat again, after the topcoat is naturally leveled on the surface, then spray the topcoat;
[0056] S7, then dry and cure the plastic chair at a temperature of 70°C for 9 minutes, and then dry at a temperature of 40°C until the moisture content is 5%.
[0057] In the step 1, the plastic chair is heated to 60° C. and kept for 2 hours.
[0058] In said step 2, clean the plastic chair with gasoline or alcohol, then rinse its surface with pure water, and finally dry it at room temperature.
[0059] In step 3, a...
PUM
Property | Measurement | Unit |
---|---|---|
Thickness | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information

- Generate Ideas
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com