A manufacturing method and technology of sleeping pillows, which are applied in the field of sleeping pillows, can solve the problems of expensive health care pillows and poor comfort in use, and achieve the effects of rapid wound healing, prevention of loss of active ingredients, and simple manufacturing methods
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0017] The health care material components include 10 parts by weight of silicone rubber, 5 parts of modified graphite, 2 parts of antioxidant, 4 parts of linear silicone oil, 1 part of nano-titanium dioxide, 1 part of nano-silver oxide, 2 parts of chitin fiber, and aloe extract 12 parts, 2 parts of Houttuynia cordata, 2 parts of lemon eucalyptus, 4 parts of desmodium.
[0018] The manufacturing method of this embodiment includes the following steps:
[0019] A. After mixing silicone rubber, modified graphite, antioxidant, linear silicone oil and nano-titanium dioxide, add it to the stirring tank and stir at a low speed. The stirring rate is 200 rpm and the stirring time is 20 minutes to obtain the mixture A;
[0020] B. After mixing Houttuynia cordata, lemon eucalyptus, and desmodium, add it to a pulverizer for pulverization, the pulverization rate is 100 rpm, and then pass through a 100-mesh sieve to obtain mixture B;
[0021] C. Add mixture B to mixture A, then add nano-si...
Embodiment 2
[0025] The health care material components include 20 parts by weight of silicone rubber, 15 parts of modified graphite, 6 parts of antioxidant, 12 parts of linear silicone oil, 6 parts of nano-titanium dioxide, 3 parts of nano-silver oxide, 9 parts of chitin fiber, and aloe extract 30 parts, 8 parts of Houttuynia cordata, 8 parts of lemon eucalyptus, and 10 parts of desmodium.
[0026] The manufacturing method of this embodiment includes the following steps:
[0027] A. After mixing silicone rubber, modified graphite, antioxidant, linear silicone oil, and nano-titanium dioxide, add it to the stirring tank and stir at a low speed. The stirring rate is 400 rpm and the stirring time is 30 minutes to obtain the mixture A;
[0028] B. After mixing Houttuynia cordata, lemon eucalyptus, and desmodium, add it to a pulverizer for pulverization, the pulverization rate is 400 rpm, and then pass through a 100-mesh sieve to obtain mixture B;
[0029] C. Add mixture B to mixture A, then a...
Embodiment 3
[0033] The health care material components include 12 parts of silicone rubber, 7 parts of modified graphite, 3 parts of antioxidant, 6 parts of linear silicone oil, 2 parts of nano-titanium dioxide, 2 parts of nano-silver oxide, 3 parts of chitin fiber, and aloe extract 14 parts, 3 parts of Houttuynia cordata, 3 parts of lemon eucalyptus, 6 parts of desmodium.
[0034] The manufacturing method of this embodiment includes the following steps:
[0035] A. After mixing silicone rubber, modified graphite, antioxidant, linear silicone oil, and nano-titanium dioxide, add it to the stirring tank and stir at a low speed. The stirring rate is 220 rpm, and the stirring time is 22 minutes to obtain the mixture A;
[0036] B. After mixing Houttuynia cordata, lemon eucalyptus, and desmodium, add it to a pulverizer for pulverization at a pulverization rate of 200 rpm, and then pass through a 100-mesh sieve to obtain mixture B;
[0037] C. Add mixture B to mixture A, then add nano-silver o...