Painting gouache paint and method for preparing same

A technology for gouache paint and painting, applied in the field of gouache paint for painting and its preparation, can solve the problems of cracking, large color difference change, mildew and the like, and achieve the effect of ensuring long-term durability, good color and luster, and not easy to mold.

Inactive Publication Date: 2018-12-25
苏州德加画材科技有限公司
View PDF3 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

This patent enhances the color and tinting strength by adding nano-pigment paste. Although it also achieves a certain weather resistance, it still has cracking, mildew, and color difference in the outdoor environment of alternating high and low temperature, alternating dry and wet, and alternating cold and heat. Defects such as large changes and poor covering power are not conducive to the application of painting gouache pigments for outdoor murals
[0004] Another example is the Chinese invention patent CN106221343A, which discloses a nanoscale weather-resistant painting gouache pigment and its preparation method, including: 20-30 parts of peach gum, 5-10 parts of pottery clay, 4-10 parts of nano-titanium dioxide, phthalocyanine green G 3- 10 parts, Fast Yellow G5-12 parts, Potassium Monododecyl Phosphate 6-15 parts, Coconut Oil Fatty Acid Diethanolamide 10-18 parts, Mannuronic Acid 2-6 parts, Fungicide 1-3 parts , 6-14 parts of guar gum, 3-9 parts of hydroxyethyl cellulose, 4-10 parts of aluminum silicate, 6-12 parts of ethylene glycol, 2-5 parts of triethanolamine, 40-80 parts of water; Although the patent has achieved certain advantages such as enhanced coverage and small color difference changes in high humidity and high temperature environments, the improvement in the stability of pigments in outdoor high and low temperature alternating, dry and wet alternating, and cold and hot environments is still small, and there are still some advantages. Cracking, mildew, etc., and there are certain discoloration problems

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Painting gouache paint and method for preparing same
  • Painting gouache paint and method for preparing same

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0026] This embodiment provides a kind of painting gouache pigment, and the raw material formula comprises: 15 parts of phthalocyanine green G, 4 parts of clay, 3 parts of nano-titanium dioxide, 3 parts of nano-zinc oxide, 4 parts of nano-calcium carbonate, 10 parts of peach gum, 5 parts of gum arabic Parts, 5 parts of ethylene glycol, 1.3 parts of potassium monolauryl phosphate, 2.7 parts of coconut oil fatty acid diethanolamide, 3.4 parts of triethanolamine, 0.15 parts of polyether modified polydimethylsiloxane, N- (β-aminoethyl)-γ-aminopropylmethyldimethoxysilane 0.15 parts, cellulose hydroxyethyl ether 0.3 parts, bactericide 2 parts and water 41 parts.

[0027] The preparation method includes: weighing the above-mentioned raw materials according to the formula ratio, mixing the phthalocyanine green G, the clay, the nano-titanium dioxide, the nano-zinc oxide, the nano-calcium carbonate, and 1 / 2 of the peach gum , 1 / 2 of the gum arabic, the polyether-modified polydimethylsil...

Embodiment 2

[0029] This embodiment provides a kind of painting gouache, and the raw material formula includes: 14 parts of phthalocyanine green G, 4 parts of pottery clay, 4 parts of nano-titanium dioxide, 3 parts of nano-zinc oxide, 4 parts of nano-calcium carbonate, 8 parts of peach gum, 7 parts of gum arabic Parts, 5 parts of ethylene glycol, 1 part of potassium monolauryl phosphate, 3 parts of coconut oil fatty acid diethanolamide, 2.2 parts of triethanolamine, 0.15 parts of polyether modified polydimethylsiloxane, N- (β-aminoethyl)-γ-aminopropylmethyl diethoxysilane 0.17 parts, cellulose hydroxyethyl ether 0.48 parts, bactericide 2 parts and water 42 parts.

[0030]The preparation method includes: weighing the above-mentioned raw materials according to the formula ratio, mixing the phthalocyanine green G, the clay, the nano-titanium dioxide, the nano-zinc oxide, the nano-calcium carbonate, and 1 / 2 of the peach gum , 1 / 2 of the gum arabic, the polyether-modified polydimethylsiloxane, ...

Embodiment 3

[0032] This embodiment provides a kind of painting gouache, and the raw material formula includes: 17 parts of phthalocyanine green G, 4 parts of pottery clay, 4 parts of nano-titanium dioxide, 4 parts of nano-zinc oxide, 4 parts of nano-calcium carbonate, 5 parts of peach gum, guar beans 9 parts of glue, 4 parts of ethylene glycol, 1.6 parts of potassium monododecyl phosphate, 2.4 parts of coconut oil fatty acid diethanolamide, 3.04 parts of triethanolamine, 0.17 parts of polyether modified polydimethylsiloxane, 0.15 parts of N-(β-aminoethyl)-γ-aminopropylmethyldimethoxysilane, 0.64 parts of cellulose hydroxyethyl ether, 2 parts of fungicide and 39 parts of water.

[0033] The preparation method includes: weighing the above-mentioned raw materials according to the formula ratio, mixing the phthalocyanine green G, the clay, the nano-titanium dioxide, the nano-zinc oxide, the nano-calcium carbonate, and 1 / 3 of the peach gum , 1 / 3 of the guar gum, the polyether-modified polydime...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
particle sizeaaaaaaaaaa
Login to View More

Abstract

The invention discloses painting gouache paint and a method for preparing the same. Raw materials for the painting gouache paint include paint color paste, pottery clay, nanometer titanium dioxide, adhesive, coalescing agents, surfactants, thickeners, wetting and dispersing agents, sterilizing agents, water, nanometer zinc oxide and nanometer calcium carbonate. The wetting and dispersing agents comprise organosilicon compounds and ethoxyl ether celluloses, molecules of the organosilicon compounds contain hydrophilic groups, and each organosilicon compound at least contains two hydrophobic groups. The method includes weighing the various raw materials according to formulas and proportions; mixing the paint color paste, the pottery clay, the nanometer titanium dioxide, the nanometer zinc oxide, the nanometer calcium carbonate, parts of the adhesive, the wetting and dispersing agents, parts of the surfactants and the water with one another to obtain mixtures; then adding the remaining adhesive, the remaining surfactants, the thickeners, the coalescing agents and the sterilizing agents into the mixtures and mixing the remaining adhesive, the remaining surfactants, the thickeners, the coalescing agents, the sterilizing agents and the mixtures with one another to obtain the painting gouache paint. The painting gouache paint and the method have the advantages that the painting gouachepaint is difficult to crack or mildew in high and low temperature alternating, dry and wet alternating and winter and summer alternating environments; excellent colors of the painting gouache paint further can be kept, and the painting gouache paint is high in covering power.

Description

technical field [0001] The invention belongs to the field of pigments, and in particular relates to the application of painting gouache paint under the phenomenon of outdoor high and low temperature alternation and dry-wet alternation, in particular to a painting gouache paint and a preparation method thereof. Background technique [0002] Gouache is the abbreviation of gouache painting. In my country, there are many names such as "propaganda color", etc. Compared with acrylic paint (or "concentrated advertising paint"), the covering power is weaker. The pigment used is usually called painting gouache paint. At the same time, there may also be defects in weather resistance, especially in the environment of alternating high and low temperature, alternating dry and wet, and alternating cold and heat, and mildew, and large color changes. [0003] For example, the Chinese invention patent CN101186782A discloses a nano-pigment-containing art gouache paint and a manufacturing metho...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C09D5/06
CPCC09D5/06
Inventor 李小福
Owner 苏州德加画材科技有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products