Device and method for controlling thicknesses of reinforced composite compressed samples
A technology for reinforcing composite materials and sample blocks, which is applied to a device for compressing sample block thickness of glass fiber reinforced composite materials, and controls the field of reinforced composite materials, which can solve the problem of high manual operation requirements, difficulty in ensuring uniformity and consistency, and affecting the adhesion of strain gauges. To ensure uniformity and consistency, avoid inability to horizontally bond, and ensure the effect of thickness uniformity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0039] In order to make the object, technical solution and advantages of the present invention clearer, the present invention will be further described in detail below with reference to the accompanying drawings and examples.
[0040] Such as figure 1 As shown, the device for controlling the thickness of the glass fiber reinforced composite material compressed sample block of the present invention includes two upper molds 1 of the same specification and size (only one upper mold is shown in the figure), two lower molds of the same specification and size 3- 1,3-2, L-shaped plate-shaped part 6, straight-shaped plate-shaped part 7, alignment plate-shaped part 11. The upper mold 1, the lower mold 3-1, 3-2, the L-shaped plate 6, the straight plate 7, and the alignment plate 11 are all made of space steel materials to ensure the stability and accuracy of the mold . The upper mold 1, the lower mold 3-1, and 3-2 are generally in the shape of a rectangular plate whose length is great...
PUM