[0042] The embodiment of the present application provides a preparation method of air cushion CC cream, including:
[0043] Raise the temperature of Phase A to 65-70°C, stir and disperse evenly;
[0044] Heat the water in phase C to 90-95°C and keep it for 20 minutes to sterilize, then add other ingredients in phase C after cooling down to 65-70°C, and stir to mix evenly;
[0045] Add phase B to the stirred phase A and continue to stir, homogenize for 3 minutes;
[0046] Add the stirred phase C into the homogenized phase AB, stir for 3-5 minutes, homogenize for 2-4 minutes, stir to defoam and cool down;
[0047] Cool down to 45-50°C, add phase D, and continue stirring until the temperature drops to 35-40°C;
[0048] Sampling inspection qualified storage.
[0049] It can be seen from the above technical solutions that the embodiment of the present application provides an air cushion CC cream and its preparation method. The air cushion CC cream includes phase A, phase B, phas...
Embodiment 1
[0052] Each component was prepared in the following parts by weight.
[0053] Phase A: 6.1 parts of mineral oil and disteardimethylammonium hectorite mixture, 6 parts of cyclopentasiloxane, 3 parts of trimethylpentaphenyltrisiloxane, 0.5 part of starch octene aluminum succinate, 3 parts polyglyceryl-3 diisostearate, polyglyceryl-6 polyhydroxystearate and C 12 -C 15 Alcohol Benzoate, 2 parts Cetyl PEG / PPG-10 / 1 Dimethicone and Cetearyl Dimethicone / Vinyl Dimethicone Blend, 3 parts phenyl trimethicone, 10 parts dioctyl carbonate, and 2.8 parts boron nitride and dimethicone mixture.
[0054] Phase B: 2 parts of titanium dioxide, 7 parts of zinc oxide, 0.05 part of Phellinus alcohol extract, and 5 parts of boron nitride, talc and polydimethylsiloxane mixture.
[0055] Phase C: 41.5 parts of water, 5.5 parts of glycerin, 0.3 parts of sodium chloride, 3.4 parts of a mixture of palmitamidopropyltrimonium chloride and propylene glycol, 6 parts of Antarctic ice sea brown algae extract...
Embodiment 2
[0059] Embodiment 2 has the same operation steps as Embodiment 1, except that the parts by weight of each component are different.
[0060] Phase A: 7.9 parts of mineral oil and disteardimethylammonium hectorite mixture, 4 parts of cyclopentasiloxane, 1 part of trimethylpentaphenyltrisiloxane, 1.8 parts of starch octene aluminum succinate, 5 parts polyglyceryl-3 diisostearate, polyglyceryl-6 polyhydroxystearate and C 12 -C 15 Alcohol Benzoate, 2 parts Cetyl PEG / PPG-10 / 1 Dimethicone and Cetearyl Dimethicone / Vinyl Dimethicone Blend, 3 parts phenyl trimethicone, 12 parts dioctyl carbonate, and 1.2 parts boron nitride and dimethicone mixture.
[0061] Phase B: 3 parts of titanium dioxide, 6 parts of zinc oxide, 0.25 part of Phellinus alcohol extract, and 6 parts of boron nitride, talc and polydimethylsiloxane mixture.
[0062] Phase C: 45.5 parts of water, 3.2 parts of glycerin, 0.3 parts of sodium chloride, 1.4 parts of palmitamidopropyltrimonium chloride and propylene glycol ...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com