[0046] A production process for an insect-proof fire hose, comprising the steps of:
[0047] a: use a circular loom to weave the braided tube 103 and the copper wire interwoven tube 104;
[0048] b: put the braided tube 103 and the copper wire interwoven tube 104 in step a into an oven for drying, the drying temperature is 50-70°C, and the drying time is 2-4 hours;
[0049] c: Prepare the following materials in parts by weight:
[0050]
[0051] d: Put the materials in step c into the mixing cylinder for stirring and mixing;
[0052] e: put the mixed materials in step d into a drying cylinder for drying, the drying temperature is 60°C, and the drying time is 2 hours;
[0053] f: Pour the dried mixture in step e into a smelting furnace for smelting;
[0054] g: Put the mixed material smelted in step f into the extruder for extrusion, after extrusion, spray 10°C circulating cooling water for cooling, and obtain the outer liner 101 semi-finished product, the inner liner 102...
Embodiment 2
[0062] A production process for an insect-proof fire hose, comprising the steps of:
[0063] a: use a circular loom to weave the braided tube 103 and the copper wire interwoven tube 104;
[0064] b: put the braided tube 103 and the copper wire interwoven tube 104 in step a into an oven for drying, the drying temperature is 60°C, and the drying time is 3 hours;
[0065] c: Prepare the following materials in parts by weight:
[0066]
[0067] d: Put the materials in step c into the mixing cylinder for stirring and mixing;
[0068] e: Put the mixed materials in step d into a drying cylinder for drying, the drying temperature is 65°C, and the drying time is 3 hours;
[0069] f: Pour the dried mixture in step e into a smelting furnace for smelting;
[0070] g: Put the mixed material smelted in step f into the extruder for extrusion, after extrusion, spray 12.5°C circulating cooling water for cooling, and obtain the outer liner 101 semi-finished product, the inner liner 102 se...
Embodiment 3
[0078] A production process for an insect-proof fire hose, comprising the steps of:
[0079] a: use a circular loom to weave the braided tube 103 and the copper wire interwoven tube 104;
[0080] b: Put the braided tube 103 and the copper wire interwoven tube 104 in step a into an oven for drying, the drying temperature is 70°C, and the drying time is 2 hours;
[0081] c: Prepare the following materials in parts by weight:
[0082]
[0083] d: Put the materials in step c into the mixing cylinder for stirring and mixing;
[0084] e: Put the mixed materials in step d into a drying cylinder for drying at a drying temperature of 70°C and a drying time of 2 hours;
[0085] f: Pour the dried mixture in step e into a smelting furnace for smelting;
[0086] g: Put the mixed material smelted in step f into the extruder for extrusion, after extrusion, spray 15°C circulating cooling water for cooling, and obtain the outer liner 101 semi-finished product, the inner liner 102 semi-fi...