Embodiment 1
[0022] An antibacterial medical dressing for promoting rapid wound healing, comprising the following raw material components in percentage by weight: 0.2% of vascular endothelial growth factor, 2% of silk fibroin aqueous solution, 2.5% of sodium alginate, 2% of sodium hyaluronate, and 3% of levofloxacin %, polyethylene glycol 400-20%, carbomer 8%, and the balance is deionized water.
[0023] Among them, vascular endothelial growth factor was purchased from Sigma Company of the United States; silk fibroin was purchased from Xi'an Four Seasons Biotechnology Co., Ltd. (molecular weight is 5000-10000, content is 98%); ; Other products and reagents are conventional commercially available.
[0024] The preparation method of the antibacterial medical dressing for promoting rapid wound healing comprises the following steps: mixing vascular endothelial growth factor, silk fibroin aqueous solution, sodium alginate, sodium hyaluronate, polyethylene glycol 400, carboxy Boomer and an appr...
Embodiment 2
[0026] An antibacterial medical dressing for promoting rapid wound healing, comprising the following raw material components in percentage by weight: vascular endothelial growth factor 0.5%, silk fibroin aqueous solution 1.8%, calcium alginate 2.8%, sodium hyaluronate 4%, Qingda Mycin 2.5%, polyethylene glycol 600-25%, carbomer 6%, and the balance is deionized water.
[0027] The preparation method of the antibacterial medical dressing for promoting rapid wound healing is the same as in Example 1.
Embodiment 3
[0029] An antibacterial medical dressing for promoting rapid wound healing, comprising the following raw material components in percentage by weight: vascular endothelial growth factor 0.4%, silk fibroin aqueous solution 1.6%, zinc alginate 3%, sodium hyaluronate 3%, molybdenum hydrochloride Cifloxacin 2%, polyethylene glycol 800 26%, carbomer 7%, and the balance is deionized water.
[0030] The preparation method of the antibacterial medical dressing for promoting rapid wound healing is the same as in Example 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com