A processing method and yarn spinning technology, which is applied in the processing field of color spinning, can solve problems such as long production cycle, difficult spinning of high-count yarn, and reduced spinnability, so as to expand the range and types, shorten the production cycle, and speed up production. The effect of the production process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A kind of raw material ratio is " 5% yellow cotton + 5% red cotton + 90% uncolored cotton " the processing method of producing gray-blue multi-color spinning yarn, comprising the following processing steps:
[0022] 1. Dyeing of yellow cotton and red cotton
[0023] Dye yellow and red cotton separately on the bulk fiber dyeing machine, and ensure uniform dyeing by controlling the amount of dye, saline and alkali, and color fixing time. The dye concentration is 0.5-1% (owf), the dosage of salt is 20-30g / L, the dosage of alkali is 10-20g / L, and the time is 45min.
[0024] 2. Cotton blending
[0025] According to the weight ratio of 5:5:90, the yellow, red, and natural color cotton are piled up on the cotton opening and cleaning machine and mixed, so that the fibers of various colors are distributed in various parts of the yarn.
[0026] 3. Spinning
[0027] The process of carding, drawing, roving, spun yarn, and doubling should adopt the spinning process with light wei...
Embodiment 2
[0035] A processing method for producing reddish-purple multi-color spinning yarn with a ratio of raw materials of "8% blue cotton sliver bucket 92% boiled and bleached cotton sliver", comprising the following processing steps:
[0036] 1. Blue cotton fiber dyeing
[0037] The blue cotton is dyed on the bulk fiber dyeing machine, and the uniformity of dyeing is ensured by controlling the amount of dye, the amount of saline and alkali, and the color fixing time. The dye concentration is 0.5-1% (owf), the amount of salt: 20-30g / L, the amount of alkali 10-20g / L, and the time is 45 minutes.
[0038] 2. Natural color cotton boiled and bleached
[0039] Wash, boil and bleach on the loose fiber dyeing machine, add hydrogen peroxide 5.5g / l, 50% concentration caustic soda 1.5g / l, multifunctional refining agent 1.5g / l, temperature 98 ℃, time 45 minutes.
[0040] 3. Cotton blending
[0041] According to the weight ratio of 8:92, the blue cotton and the boiled and bleached cotton are p...
Embodiment 3
[0051] A processing method for producing blue-black multi-color spinning yarn with a ratio of raw materials of "7% black cotton + 93% natural color cotton", comprising the following processing steps:
[0052] 1. Black cotton dyeing
[0053] Black cotton is dyed on a bulk fiber dyeing machine, and uniform dyeing is ensured by controlling the amount of dye, saline and alkali, and color fixation time. The dye concentration is 0.5-1% (owf), the dosage of salt is 20-30g / L, the dosage of alkali is 10-20g / L, and the time is 45min.
[0054] 2. Cotton blending
[0055] According to the weight ratio of 7:93, the black cotton and the natural color cotton are piled up on the cotton opening and cleaning machine to mix the cotton, so that the fibers of various colors are distributed in various parts of the yarn.
[0056] 3. Spinning
[0057] The process of carding, drawing, roving, spun yarn, and doubling should adopt the spinning process with light weight, slow speed and easy transfer. ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com