Curtain coating method and curtain coating apparatus
A curtain coating and curtain technology, which is applied to the surface coating liquid device, coating, etc., can solve the problems of undisclosed curtain edge rail coating liquid residue and auxiliary liquid removal
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0206] in figure 2 The bottom of the curtain guide rail of the sliding curtain coating device shown in is installed in a rotatable manner Figure 10A with 10B The disc-shaped claw 102 is shown in, while the mandrel is fixed at the center of the claw. Then, the thermal recording layer coating liquid prepared according to the following formula was applied to the top of the web (paper), the coating speed was 400m / min, the coating width was 250mm and the flow rate of the coating liquid (from the nozzle slit Spray) is 3,000 g / min. At this time, the disc-shaped claws are made of stainless steel and have a radius of 20 mm and a thickness of 0.18 mm. The amount of auxiliary liquid (water) flowing along the curtain rail is 30 cc / min, and is used to recover the auxiliary liquid. The suction pressure of the vacuum unit is -8kpa. Likewise, the claw portion 102 is manufactured to protrude 2 mm from the curtain liquid film contact surface of the porous member 13 (which is made of ceramic a...
Embodiment 2
[0215] Except that the radius of the disc-shaped claw portion 102 was changed from 20 mm to 5 mm, the thermosensitive recording layer coating liquid was applied to the coil in the same manner as in Example 1. The results are shown in Table 1-A.
Embodiment 3
[0217] In addition to using Figure 5A to 5C The sliding curtain coating device shown in-in which a flat plate-shaped claw 101 (which is made of stainless steel and has a thickness of 0.18mm, a length of 60mm with respect to its moving direction and a width of 30mm) is clamped in the drive Between the rubber rollers 14 and configured to move back and forth (at a rate of 0.005 m / sec)—except, the thermosensitive recording layer coating liquid was applied to the coil in the same manner as in Example 1. The results are shown in Table 1-A.
PUM