A technology of metal powder and multi-layer metal, which is applied in the production field of multi-layer metal mesh and metal powder composite filter, can solve the problems of low pressure, failure of the filter system, production difficulties, etc., and achieve low filtration resistance and high filtration accuracy , the effect of strong pressure bearing capacity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] Example 1: Take one sheet of 100 mesh with a length of 1000mm and a width of 500mm, two sheets of 40 mesh, and two sheets of 12 mesh. Layers of wire mesh are arranged neatly and superimposed, and then boundary butt welding is performed. Put it into a vacuum furnace after welding, and carry out sintering treatment at 1000-1600°C to obtain a support layer; after cooling and taking out the support layer, take 1-2 kg of stainless steel 316L powder with a particle size of 100-200 mesh, add 0.1%- 20% molding agent, mixed in the mixing equipment for 1-3 hours and taken out, the mixing equipment is V-shaped mixing equipment, double cone mixer or ball mill, and then cast on the re-sintered 5-layer mesh support layer The mixed stainless steel powder has a thickness of 1-5mm, and then the composite structure is put into a vacuum furnace, sintered at 1000-1600°C for secondary sintering treatment, and after cooling and taken out, a composite filter of multi-layer metal mesh and meta...
Embodiment 2
[0024] Example 2: Take 1 sheet of 500 mesh, 2 sheets of 40 mesh, and 2 sheets of 12*64 mesh with a length of 1000mm and a width of 500mm. From top to bottom, they are 500 mesh, 40 mesh, 40 mesh, 12*64 mesh, 12* 64 mesh, the 5 layers of wire mesh are arranged neatly and superimposed, and then boundary welding is performed. Put it into a vacuum furnace after welding, and carry out sintering treatment at 1000-1600 ° C to obtain a support layer; take out the support layer after cooling, and then take 1-2 kg of stainless steel 316L powder with a particle size of 400-500 mesh, add 0.1 %-20% molding agent, mixed in the mixing equipment for 1-3 hours and then taken out, the mixing equipment is V-type mixing equipment, double cone mixer or ball mill, and then supported by re-sintered 5-layer mesh Cast the mixed stainless steel powder on the layer with a thickness of 1-5mm, then put the composite structure into a vacuum furnace, sinter at 1000-1600°C for secondary sintering treatment, t...
Embodiment 3
[0025] Embodiment 3: Take the metal nickel mesh with a length of 1000mm and a width of 500mm, wherein 1 sheet of 100 mesh, 1 sheet of 40 mesh, and 2 sheets of 10 mesh, from top to bottom are successively 100 mesh, 40 mesh, 10 mesh, and 10 mesh. These 4 layers of wire mesh are neatly arranged and stacked, and then boundary welding is performed. Put it into a vacuum furnace after welding, and carry out sintering treatment at 1000-1600 ° C to obtain a support layer; take out the support layer after cooling, and then take 1-2 kg of metal nickel powder with a particle size of 100-200 mesh, add 0.1 %-20% molding agent, mixed in the mixing equipment for 1-3 hours and then taken out, the mixing equipment is V-shaped mixing equipment, double cone mixer or ball mill, and then supported by the re-sintered 4-layer mesh Cast the mixed metal nickel powder on the layer with a thickness of 1-5mm, then put the composite structure into a vacuum furnace, sinter at 1000-1600°C for secondary sinte...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com