Additive for improving appearance of paint and synthesis method thereof
A synthesis method and additive technology, applied in the direction of coating, etc., can solve problems such as paint surface defects, unfavorable corporate reputation, delay in delivery, etc., and achieve the effects of improving gloss, eliminating orange peel phenomenon, and increasing leveling time
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] A method for synthesizing an additive for improving the appearance of a paint, the method comprising the following steps:
[0031] (1) Dosing according to the following components and contents: 10kg of surface control agent, 40kg of slow-drying solvent, wherein, the surface-controlling agent is an acrylate polymer, and the slow-drying solvent is isophorone;
[0032] (2) Put 80% of the slow-drying solvent into the dispersion container according to the formula requirements, control the temperature at 20°C, stir at 100 rpm, and stir at a slow speed for 10 minutes;
[0033] (3) keep stirring and put the surface control agent into the dispersing container in turn, the stirring speed is 200rpm and continue to stir for 30min;
[0034] (4) Use the remaining slow-drying solvent to adjust the content of the surface control agent to a theoretical value of 7 wt%, stir slowly at a stirring speed of 100 rpm for 30 minutes, and obtain the product after filtration.
Embodiment 2
[0036] A method for synthesizing an additive for improving the appearance of a paint, the method comprising the following steps:
[0037] (1) According to the following components and content batching: 12kg of surface control agent, 65kg of slow-drying solvent, wherein, the surface control agent is a fluorine-containing acrylate polymer, and the slow-drying solvent is a mixture of isophorone and dimethyl adipate. mixture;
[0038] (2) Put 85% of the slow-drying solvent into the dispersion container according to the formula requirements, control the temperature at 25°C, stir at 120rpm, and stir at a slow speed for 8 minutes;
[0039] (3) keep stirring and put the surface control agent into the dispersing container in turn, the stirring speed is 240rpm and continue to stir for 20min;
[0040] (4) Use the remaining slow-drying solvent to adjust the content of the surface control agent to a theoretical value of 7.5 wt%, stir slowly at a stirring speed of 150 rpm for 20 min, and o...
Embodiment 3
[0042] A method for synthesizing an additive for improving the appearance of a paint, the method comprising the following steps:
[0043] (1) Dosing according to the following components and content: 15kg of surface control agent, 50kg of slow-drying solvent, wherein, the surface control agent is a mixture of acrylate polymer and fluorine-containing acrylate polymer, and the slow-drying solvent is propylene glycol methyl ether acetate ;
[0044] (2) Put 85% slow-drying solvent into the dispersion container according to the formula requirements, control the temperature at 25°C, stir at 150rpm, and stir at a slow speed for 10min;
[0045] (3) keep stirring and put the surface control agent into the dispersing container in turn, the stirring speed is 260rpm and continue to stir for 15min;
[0046] (4) Use the remaining slow-drying solvent to adjust the content of the surface control agent to a theoretical value of 7.8 wt%, stir slowly at a stirring speed of 100 rpm for 30 min, a...
PUM