Embodiment 1
[0033] (1) Synthesis of sulfonated graphene
[0034] 37.5 mg of graphite oxide was dispersed in 37.5 g of water. Then a brown graphene oxide suspension was obtained after ultrasonication for 1 h.
[0035] Pre-reduction: first use 5wt% sodium carbonate solution to adjust the pH of the above-mentioned graphene oxide suspension to 9, mix 300mg NaBH 4 Dissolve in 7.5g water, and then add NaBH 4 The solution was added to the graphene oxide suspension. The mixture was stirred continuously at 80 °C for 1 h. The reduction process was carried out under nitrogen atmosphere. The suspension turned from coffee color to black. Aggregation was observed after the reduction reaction, and after centrifugation and washing with water for 2 to 3 times, the partially reduced graphene oxide was dispersed in 37.5 g of water by ultrasound to obtain a suspension;
[0036] Sulfonation: 23mg p-aminobenzenesulfonic acid and 9mg sodium nitrite in 5g water and 0.25g 1mol L -1React in HCl, form diazon...
Embodiment 2
[0049] (1) Synthesis of sulfonated graphene
[0050] 37.5 mg of graphite oxide was dispersed in 37.5 g of water. Then a brown graphene oxide suspension was obtained after ultrasonication for 1 h.
[0051] Pre-reduction: first adjust the pH of the above-mentioned graphene oxide suspension to 10 with 5wt% sodium carbonate, mix 300mg NaBH 4 Dissolve in 7.5g water, and then add NaBH 4 The solution was added to the above graphene oxide suspension. The mixture was stirred continuously at 80 °C for 1 h. The reduction process was carried out under nitrogen atmosphere. The suspension turned from coffee color to black. Aggregation was observed after the reduction reaction, and after centrifugation and washing with water for 2 to 3 times, the partially reduced graphene oxide was dispersed in 37.5 g of water by ultrasound to obtain a suspension;
[0052] Sulfonation: 23mg p-aminobenzenesulfonic acid and 9mg sodium nitrite in 5g water and 0.25g 1mol L -1 React in HCl to form diazoni...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com