Sol soaked glass wrapped layer soft magnetism composite material and preparation method thereof

A soft magnetic composite material, glass coating technology, applied in the direction of inorganic material magnetism, etc., can solve the problems of high temperature resistance, serious environmental pollution, restricting the development and application of soft magnetic composite materials, etc., to improve magnetic properties and eliminate internal stress. Effect

Active Publication Date: 2014-11-12
HARBIN INST OF TECH
View PDF4 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

For the existing organic-coated soft magnetic composite materials, a pressure greater than 800 MPa needs to be applied during its preparation to achieve the required compaction density, but at the same time it must satisfy good saturation magnetic induction and magnetic permeability. rate, it is necessary to anneal the soft magnetic composite material containing the organic coating layer to remove the residual stress of the material, because the organic coating layer is usually not resistant to high temperature, so it is difficult to effectively remove the residual stress
For the soft magnetic composite material of the existing inorganic cladding layer, the insulation of the cladding layer cannot meet the requirements, and the existing cladding layer containing P or S is serious to the environmental pollution, so the use of SiO 2 , MgO, SiO 2 Mixture with water, Al 2 o 3 mixed with water, ZrO 2 The inorganic insulating layer prepared by mixing with water, mica powder and water is used as the inorganic coating layer, and the inorganic insulating layer is generally stable at high temperature, which overcomes the disadvantage that the organic coating layer is usually not resistant to high temperature
However, the existing inorganic insulating layer also has disadvantages. The thermal expansion coefficient of the inorganic insulating layer and the magnetic powder differ greatly, and the thermal expansion coefficient of the inorganic insulating layer itself cannot be changed. In an environment with a large temperature difference or during long-term use, the magnetic powder will Thermal stress is generated inside, which leads to the failure of the soft magnetic composite material coated with inorganic materials to have excellent magnetic properties.
These problems restrict the development and application of soft magnetic composite materials.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Sol soaked glass wrapped layer soft magnetism composite material and preparation method thereof
  • Sol soaked glass wrapped layer soft magnetism composite material and preparation method thereof
  • Sol soaked glass wrapped layer soft magnetism composite material and preparation method thereof

Examples

Experimental program
Comparison scheme
Effect test

specific Embodiment approach 1

[0031] Embodiment 1: The sol-infiltrated glass-coated soft magnetic composite material provided in this embodiment is composed of magnetic powder, a silicon dioxide layer coated with magnetic powder, a glass layer coated outside the silicon dioxide layer, and a glass sol infiltrated Layer composition; wherein, the magnetic powder is one or a combination of magnetic metal powder, magnetic metal alloy powder and magnetic metal compound powder.

[0032] The sol-infiltrated glass-clad soft magnetic composite material provided in this embodiment can adjust the composition and proportion of the glass layer according to the coefficient of thermal expansion. The thermal expansion coefficients of the two substances in one material do not match, and internal stress is easily generated inside the material when the temperature changes, which in turn reduces the magnetic properties of the soft magnetic composite material. Therefore, in the selection of the cladding layer, the thermal expan...

specific Embodiment approach 2

[0035] Specific embodiment two: the difference between this embodiment and specific embodiment one is: the magnetic powder is Fe powder, Ni powder, Co powder, iron alloy powder, nickel alloy powder, cobalt alloy powder, iron-containing oxide powder, nickel-containing oxide One or a combination of powders and cobalt oxide powders are magnetic.

[0036] The iron alloy powder described in this embodiment is an alloy powder composed of iron element and one or more elements, and the mass fraction of iron is the largest, wherein the iron alloy powder can be Fe-Si-Al powder, Fe-Ni-Mo powder, Fe-Ni powder, Fe-Cu-Nb-Si-B powder, Fe-Pt powder, Fe-Ni-Cr powder, Fe-Zn powder, La-Co-Fe powder, Pb-Fe powder, W-Ni-Fe powder Powder and Zr-Ni-Sn-Fe powder or a combination of several of them.

[0037] The nickel alloy powder described in this embodiment is an alloy powder composed of nickel element and one or more elements, and the mass fraction of nickel is the largest, wherein the nickel all...

specific Embodiment approach 3

[0039] Specific implementation mode three: The preparation method of the sol-infiltrated glass-clad soft magnetic composite material provided in this implementation mode is specifically completed according to the following steps:

[0040] 1. Put the magnetic powder into the cleaning agent and ultrasonicate at a frequency of 24KHz to 35KHz for 10min to 20min, filter to obtain clean magnetic powder, add ethanol and oleic acid to the clean magnetic powder, and use ammonia water with a concentration of 20% to 30% by mass to dissolve the solution Adjust the pH value to 8.5-9.5, ultrasonically disperse at a frequency of 24KHz-35KHz for 1-2 hours or stir at a speed of 600r / min-1200r / min for 1-2 hours to obtain a solid-liquid mixture;

[0041] Among them, the mass ratio of oleic acid and magnetic powder is (0.03-0.2): 1, the volume ratio of oleic acid and ethanol is 1: (40-75), and the magnetic powder is magnetic metal powder, magnetic metal alloy powder and One or a combination of se...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
breaking strengthaaaaaaaaaa
Login to view more

Abstract

The invention discloses a sol soaked glass wrapped layer soft magnetism composite material and a preparation method thereof and relates to a soft magnetic material and a preparation method thereof. By means of the sol soaked glass wrapped layer soft magnetism composite material and the preparation method thereof, the problems that thermal expansion coefficients of inorganic insulating layers and magnetic powder are large in difference, and the thermal expansion coefficients of inorganic insulating layers are invariable are solved. The sol soaked glass wrapped layer soft magnetism composite material is composed of magnetic powder, a silica layer wrapped with magnetic powder, a glass layer wrapped outside the silica layer and a glass sol infiltration layer. The preparation method includes: 1, pretreating the magnetic powder; 2, wrapping the silica layer on the surface of the magnetic powder; 3, wrapping the glass layer outside the silica layer; 4, preparing a blank of soft magnetic composite materials; 5, performing infiltration on the blank of the soft magnetic composite materials through glass sol; and 6, preparing the soft magnetic materials.

Description

technical field [0001] The invention relates to a preparation method of a soft magnetic material. Background technique [0002] Soft magnetic composite material refers to a type of soft magnetic material in which magnetic powders are independent of each other and connected by insulating layer materials. The outstanding advantages of this soft magnetic composite material are low iron loss and three-dimensional isotropic properties under AC magnetic field. Therefore, many components that are difficult to realize with conventional soft magnetic materials can be prepared, and have been used in switched reluctance, resonant inductors, anti-lock brake sensors, electromagnetic drives, brushless DC motors, rotating machinery, low-frequency filters and other fields. The preparation process of soft magnetic composite materials is usually to coat the surface of metal or alloy magnetic powder with an insulating layer of inorganic and organic matter, or to form a composite soft magnetic...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Patents(China)
IPC IPC(8): H01F1/33H01F1/24B22F1/02
Inventor 武高辉丁伟姜龙涛
Owner HARBIN INST OF TECH
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products