preparation example 1
[0049] Coated nano-Fe 3 O 4 Granule preparation
[0050] (1) Weigh 2.0 g FeCl 2 4H 2 O and 6 g FeCl 3 ·6H 2 O was placed in a three-necked flask, added 400 g of diethylene glycol, stirred to dissolve the two, then 2.5 g of NaOH was dissolved in 120 g of diethylene glycol, slowly added dropwise to the above-mentioned three-necked flask, stirred at room temperature for 2 h, and then The temperature was raised to 230°C within 1.5 h, and the reaction was carried out at this temperature for 2 h, and then cooled to room temperature. A black solid was obtained by centrifugation, and the black solid was washed successively with a mixed solution of ethanol / ethyl acetate at a volume ratio of 1:1, ethanol and deionized water, and the obtained black solid was dried in a vacuum oven at 50 °C for 6 h , to obtain the base core nano-Fe 3 o 4 Particles, observed by electron microscope, have an average particle size of about 10 nm.
[0051] (2) 50 mg base-core nano-Fe 3 o 4 ...
preparation example 2
[0055] Laccase coated nano Fe 3 O 4 immobilization on particles
[0056] SiO obtained above 2 Coated nano-Fe 3 o 4 50 mg of particles were dispersed in 60 mL of deionized water under ultrasonic conditions, then 30 mg of laccase (E.C.1.10.3.2) and 4 mL of 50 mmol / L succinic acid buffer solution were added, and after stirring for 3 hours, 5 mL of 2.5% succinic acid was added dropwise. Aqueous glutaraldehyde solution was used as a cross-linking agent, stirred at room temperature for 8 h in an argon atmosphere, then placed on a magnet, poured out the supernatant, and separated to obtain a black solid, which was washed with deionized water until the washing liquid had no UV absorption , and the resulting solid was vacuum-dried at room temperature for 12 h to obtain laccase-immobilized SiO 2 Coated nano-Fe 3 o 4 particles.
[0057] In addition to the above "SiO 2 Coated nano-Fe 3 o 4 particles" replaced with "TiO 2 Coated nano-Fe 3 o 4 Particles”, obtained lac...
Embodiment 1
[0061] Weigh out laccase-immobilized SiO 2 Coated nano-Fe 3 o 4 Mix 100 mg of particles, 10 mg of copper particles with a particle size of 100 nm, and 5 mg of additives evenly. The additives include 4 mg of calcium carbonate and 1 mg of magnesium carbonate to obtain a sewage treatment agent. The sample number is 1.
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com