Preparation method of complex leather dye
A dye and leather technology, applied in the field of composite leather dye preparation, can solve the problems of poor leather affinity, poor solubility, and poor levelness, and achieve high leather affinity, good solubility, and good levelness. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0033] In this embodiment, acid black NT (C.I.Acid Black210) is used as the original dye.
[0034] Add 2000Kg of acid black NT (C.I.Acid Black210) to 10,000L of water, raise the temperature to 60°C, stir to completely dissolve, add 40Kg of polyethylene glycol 400, add 4Kg of hydroxypropyl methylcellulose, and add 50Kg of pentaethylenehexamine, Add 30Kg of tetramethylguanidine, add 50Kg of dispersant NNO, keep warm for 1 hour, and spray dry to obtain composite leather dye.
Embodiment 2
[0036] In this example, the selected primary dye is acid brown SG (C.I.Acid Brown348).
[0037] Add 1600Kg of acid brown SG (C.I.Acid Brown348) to 10,000L of water, raise the temperature to 70°C, stir to dissolve completely, add 35Kg of polyethylene glycol 200, 30Kg of polyethylene glycol 600, add 1Kg of hydroxymethyl cellulose, hydroxyethyl Base cellulose 2Kg, add tetraethylenepentamine 20Kg, pentaethylenehexamine 20Kg, add tetramethylguanidine 20Kg, add dispersant MF50Kg, keep warm for 1 hour, spray dry to get composite leather dye.
Embodiment 3
[0039] In this example, the selected primary dye is a compound of acid black NT (C.I.Acid Black210), acid black NBG (C.I.Acid Black234), and direct black HEF (C.I.Direct Black168).
[0040] In 10000L water, add acid black NT (C.I.Acid Black210) 2000Kg, acid black NBG (C.I.Acid Black234) 800Kg, direct black HEF (C.I.Direct Black168) 200Kg, raise the temperature to 60°C, stir and dissolve completely, then add 40Kg polyethylene glycol Alcohol 400, 40Kg polyethylene glycol 600, add hydroxypropyl methylcellulose 3Kg, hydroxyethyl cellulose 2Kg, add triethylenetetramine 30Kg, pentaethylenehexamine 30Kg, add tetramethylguanidine 30Kg, add dispersant NNO60Kg, heat preservation reaction for 1 hour, and spray drying to obtain a composite leather dye.