A compound type, grinding block technology, applied in manufacturing tools, metal processing equipment, grinding/polishing hand tools, etc., can solve the problems of unsatisfactory polishing effect, low grinding efficiency, poor wear resistance, etc. Good effect, high grinding efficiency and good wear resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
no. 1 example
[0033] see figure 1 - Figure 15 , the resin-metal composite elastic grinding block, including abrasive layer 1, elastic layer 2 and clamping head 3, is characterized in that abrasive layer 1 and elastic layer 2 are arranged on clamping head 3 in sequence, abrasive layer 1 and elastic layer 2 The surface of the abrasive layer 1 has a circular arc structure, and the abrasive layer 1 is connected with a number of grinding blocks through a Velcro belt (hook surface). The grinding blocks are metal-bonded diamond segments 1.1, and the outer periphery is wrapped with a resin material 1.2. The surface of the grinding block has a circular arc structure, and the number is 9-24. The elastic layer 2 is soft rubber or soft plastic elastic body, and is bonded with the clamping head 3 .
[0034] A mold for making the above-mentioned resin-metal composite elastic abrasive block, which respectively includes a block making mold for making the above-mentioned metal-bonded diamond segment 1.1,...
no. 2 example
[0042] It differs from the first embodiment in that:
[0043] The manufacturing method of the abrasive material layer 1: fix the tooth-shaped forming mold body 8 on the mounting part 7.1 of the abrasive layer manufacturing mold frame 7, and put one of the above-mentioned The metal-bonded diamond segment 1.1 formed by sintering is poured into epoxy resin, and put into a Velcro tape (with the hook side facing the resin), covered with the upper template 9, and then placed at room temperature for natural curing for 12 hours, and then released from the mold ;
[0044] Other unmentioned parts are the same as the first embodiment.
no. 3 example
[0046] It differs from the first embodiment in that:
[0047] The manufacturing method of the abrasive material layer 1: fix the tooth-shaped forming mold body 8 on the mounting part 7.1 of the abrasive layer manufacturing mold frame 7, and put one of the above-mentioned The metal-bonded diamond segment 1.1 formed by sintering is poured into unsaturated polyester resin, and put into a Velcro tape (the hook side faces the resin), and the upper template 9 is covered, and then placed at room temperature to naturally cure for about 1 hour, and then Unmold it out.
[0048] Other unmentioned parts are the same as the first embodiment