A production method and stretch-resistant technology, applied in special leather manufacturing, small raw hide/big raw hide/leather/fur treatment, small raw hide/large raw hide/leather/fur mechanical treatment, etc., can solve the problem of poor stretch resistance of leather , easy deformation and other problems, to achieve the effect of high tensile performance and not easy to deform
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The invention provides a production method of stretch-resistant leather, which comprises:
[0026] Prepare the leather material, shave it to an even thickness of 1.6-1.8 mm, the leather body is full, hairy, soft and hard.
[0027] Primer coating process: Take 80 parts by mass of water, heat it to 10-25 degrees Celsius, add 90-110 parts by mass of water-based discoloration wax, stir for 1-2 minutes, then add 90-110 parts by mass of burnt black wax, stir for 1-2 minutes, Then add 12-40 parts by mass of soft casein, stir for 1-2 min, then add 30-50 parts by mass of acrylic resin, which is fully dissolved; spread the leather on the conveyor belt of the roller coating machine, and the roller speed 28 revolutions per second, the conveying speed of the conveyor belt is 0.1 meters per second, roll coating once, and the coating dosage is 20~25g / square foot;
[0028] Hanging drying process: hang drying at room temperature of 10-30 degrees Celsius for 6 hours;
[0029] Polishing...
Embodiment 2
[0033] The invention provides a production method of stretch-resistant leather, which comprises:
[0034] Prepare the leather material, shave it to an even thickness of 1.6-1.8 mm, the leather body is full, hairy, soft and hard.
[0035] Primer coating process: take 80 parts by mass of water, heat to 10~25 degrees Celsius, add 95 parts by mass of water-based discoloration wax, stir for 1~2min, then add 100 parts by mass of burnt black wax, stir for 1~2min, then add 40 parts by mass The soft casein in parts by mass is stirred for 1-2 min, and then 40 parts by mass of acrylic resin is added to fully dissolve it; the leather is spread flat on the conveyor belt of the roller coating machine, the drum speed is 30 revolutions per second, and the transmission of the conveyor belt The speed is 0.1 m / s, roll coating once, and the amount of paint is 25g / square foot;
[0036] Hanging drying process: hang drying at room temperature of 10-30 degrees Celsius for 8 hours;
[0037] Polishin...
Embodiment 3
[0041] The invention provides a production method of stretch-resistant leather, which comprises:
[0042] Prepare the leather material, shave it to an even thickness of 1.6-1.8 mm, the leather body is full, hairy, soft and hard.
[0043] Primer coating process: Take 80 parts by mass of water, heat it to 10~25 degrees Celsius, add 100 parts by mass of water-based discoloration wax, stir for 1~2min, then add 110 parts by mass of burnt black wax, stir for 1~2min, then add 30 parts by mass Soft casein in parts by mass, stirred for 1-2 min, and then added 50 parts by mass of acrylic resin to fully dissolve it; spread the leather on the conveyor belt of the roller coating machine, the drum speed is 28 revolutions per second, and the transmission of the conveyor belt The speed is 0.12 meters per second, roll coating once, and the amount of paint is 23g / square foot;
[0044] Hanging drying process: hang drying at room temperature of 10-30 degrees Celsius for 12 hours;
[0045] Polis...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com