Preparation method of magnetic silver phosphate
A silver phosphate and magnetic technology, applied in the field of photocatalysis, can solve the problems of wide promotion, narrow light response range, low quantum efficiency, etc., and achieve the effects of good development prospects, simple preparation process and high recycling rate.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0021] A preparation method of magnetic silver phosphate, comprising the following steps:
[0022] 1) Mix silver nitrate aqueous solution with a concentration of 0.1~1mol / L and ammonia water with a concentration of 1-3% to make a silver ammonia solution, the concentration of the dilute ammonia water is 1-3%; mix the silver ammonia solution and polyvinylpyrrolidone Mix the PVP evenly, add 0.01~1g of iron ferric oxide nanoparticles with a particle size of 1-10nm, and ultrasonicate for 20min in an ultrasonic machine with an ultrasonic frequency of 50HZ to form the first mixed solution;
[0023] 2) Mix the disodium hydrogen phosphate aqueous solution with a concentration of 0.01~0.1mol / L and PVP evenly to form the second mixed solution;
[0024] 3) Adding the second mixed solution dropwise to the first mixed solution under stirring conditions to obtain a yellow-brown turbid solution;
[0025] 4) Put the yellowish-brown turbid liquid in a centrifuge tube, place it in a centrifuge ...
Embodiment 1
[0032] 1. Preparation of silver phosphate photocatalyst:
[0033] 1. Add silver nitrate to ionized water to prepare a silver nitrate aqueous solution with a concentration of 0.1-1mol / L. Dilute ammonia water (2%) is prepared by adding 1ml of laboratory concentrated ammonia water (25% by mass) to 10ml of distilled water.
[0034] 2. Take 30mL of silver nitrate aqueous solution, add dilute ammonia water drop by drop, shake while dripping, until the initial precipitate is just dissolved, and prepare silver ammonia solution. The reaction process is as follows:
[0035] .
[0036] Add 0.01-1g of PVP to the silver-ammonia solution, stir evenly, then add 0.01-1g of nano iron ferric oxide with a particle size of 1-10nm, and ultrasonically form the first mixed solution. The PVP concentration in the first mixed solution is: 0.5~20g / L.
[0037] 3. Add disodium hydrogen phosphate to ionized water to prepare an aqueous solution of disodium hydrogen phosphate with a concentration of 0.0...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com