A raw material and solvent technology, applied in the field of Grace and its continuous antique American coating process, can solve the problems of affecting production efficiency, large labor demand, long coating time, etc., and achieve high construction efficiency, high coating efficiency, good adhesion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] In an embodiment, the mass parts of each raw material of Grace is
[0032] 30 parts of stuffing;
[0033] 20 parts of pigment;
[0034] 18 parts of solvent;
[0035] 30 parts of water;
[0036] Auxiliary 2 parts.
[0037] The filler is a combination of any mixing ratio of talcum powder and silicon powder.
[0038] The pigment is a composition of any mixing ratio in the inorganic iron oxide color paste or color essence.
[0039] The solvent is a composition of any mixing ratio of propylene glycol, glycerol, propylene glycol methyl ether, and dipropylene glycol methyl ether.
[0040] The auxiliary agent is a composition of any mixing ratio among fumed silica, bentonite and water-based thixotropic agent.
[0041] Preparation of Grace:
[0042] 1) Partial raw material mixing: According to the raw material formula of Grace, put 8 parts of water, 2 parts of solvent, and 2 parts of additives into the reactor, and disperse for 1 hour under the stirring of the mixer at th...
Embodiment 2
[0056] In an embodiment, the mass parts of each raw material of Grace is:
[0057] Filling 20 parts;
[0058] 20 parts of pigment;
[0059] 30 parts of solvent;
[0060] 25 parts of water;
[0061] Auxiliary 5 parts.
[0062] The filler can be any combination of talcum powder and silica micropowder.
[0063] The pigment can be any combination of organic color paste or color essence.
[0064] The solvent can be any combination of dipropylene glycol butyl ether and propylene glycol methyl ether acetate.
[0065] The auxiliary agent can be composed of fumed silica and water-based thixotropic agent in any mixing ratio.
[0066] Preparation of Grace:
[0067]1) Mixing of some raw materials: According to the raw material formula of Grace, put 6 parts of water, 3 parts of solvent, and 5 parts of additives into the reactor, and disperse for 1.5 hours under the stirring of the mixer at the speed of 1000r / s;
[0068] 2) Add filler: After the raw materials in step 1) are disperse...