Tensile composite polyester fiber
A composite fiber, anti-stretch technology, applied in the field of polyester, can solve the problems of damage to clothing size, fabric elongation, poor tensile properties of outerwear fabrics, etc., to achieve the effect of improving tensile properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0011] Including: mixed components and anti-stretch components, proportioned according to mass fraction: the content of the mixed components accounts for 65%, the content of the anti-stretch components accounts for 35%, and the mixed components are composed of polyester resin and polypropylene It is made of mixed resins, and the ratio is made according to the mass fraction: the content of the polyester resin accounts for 60%, the content of the polypropylene resin accounts for 40%, and the anti-stretching agent is obtained by high-temperature fusion of phenolic resin and epoxy resin into, proportioning according to the mass fraction: the content of the phenolic resin is 50%, and the content of the epoxy resin is 50%.
Embodiment 2
[0013] Including: mixed components and anti-stretch components, proportioned according to mass fraction: the content of the mixed components accounts for 75%, and the content of the anti-stretch components accounts for 25%. The mixed components are composed of polyester resin and polypropylene It is made of mixed resins, and the ratio is made according to the mass fraction: the content of the polyester resin accounts for 70%, the content of the polypropylene resin accounts for 30%, and the anti-stretching agent is obtained by high-temperature fusion of phenolic resin and epoxy resin into, proportioning according to the mass fraction: the content of the phenolic resin is 60%, and the content of the epoxy resin is 40%.
Embodiment 3
[0015] Including: mixed components and anti-stretch components, proportioned according to mass fraction: the content of the mixed components accounts for 70%, the content of the described anti-stretch components accounts for 30%, and the mixed components are composed of polyester resin and polypropylene It is made of mixed resins, and the ratio is made according to the mass fraction: the content of the polyester resin accounts for 65%, the content of the polypropylene resin accounts for 35%, and the anti-stretch agent is obtained by high-temperature fusion of phenolic resin and epoxy resin into, proportioning according to the mass fraction: the content of the phenolic resin is 55%, and the content of the epoxy resin is 45%.
[0016] Different from the prior art, the present invention discloses a stretch-resistant polyester composite fiber, the manufacturing process of which is as follows: first, put the phenolic resin and epoxy resin in the above ratio into a heating electric f...
PUM

Abstract
Description
Claims
Application Information

- Generate Ideas
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com